UNS N10629 Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n10629 pipe in China. If you're going to wholesale high quality uns n10629 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
N10629 alloy has good forming and welding properties and can be welded by all common welding methods. Although oxyacetylene welding and submerged arc welding are not recommended for parts used in corrosive environments, N10629 alloy can maintain excellent toughness when exposed to medium temperatures for a moment. When exposed to 700℃ for a short time, N10629 alloy is very easy to embrittle, while N10629 shows significant anti-embrittlement ability, which makes the alloy very suitable for being made into complex forming device parts.
In general, UNS N10629 pipe is a high-performance material developed for specific industrial needs. It not only overcomes some defects of traditional B2 alloy by optimizing chemical composition and processing flow, but also provides excellent corrosion resistance and processing flexibility, making it extremely widely used in harsh industrial environments.
N10629 alloy shows good corrosion resistance to hydrochloric acid at any temperature and concentration, and is also suitable for sulfuric acid, acetic acid, formic acid, phosphoric acid and other non-oxidizing media. Compared with B2 alloy, its thermal stability has been significantly improved, and it shows high resistance to pitting corrosion, stress corrosion cracking, knife-shaped corrosion and heat-affected zone corrosion of welding. The tendency to form harmful phases between metals is very small, which means that N10629 has greater toughness than B2 alloy during the heating process and subsequent various thermal cycles.
|
Chemical Properties |
|||||||||||
|
C |
Mn |
P |
S |
Si |
Cr |
Mo |
Ni |
Cu |
V |
Cb |
Ti |
|
0.01 Max |
3.0 Max |
0.030 Max |
0.010 Max |
0.10 Max |
1.0-3.0 |
27.0-32.0 |
65.0 Min |
0.20 Max |
0.20 Max |
0.20 Max |
0.20 Max |
|
Al |
W |
Co |
Ta |
Fe |
Zr |
Ni+Mo |
|||||
|
0.50 Max |
3.0 Max |
3.0 Max |
0.20 Max |
1.0-3.0 |
0.10 Max |
94.0-98.0 |
|||||
|
Mechanical Properties |
||
|
Yeild strength |
Tensile strength |
Elongation |
|
Min 0.2% Mpa |
Min Mpa |
Min % |
|
350 |
760 |
40 |
|
Physical Properties |
|||||
|
Density |
Elastic Modulus |
Mean Coefficient of Thermal |
Thermal Conductivity |
Specific Heat |
Electrical Resistivity |
|
(Kg/m 3 ) |
(Gpa) |
Expansion( μ m/m/°C) |
(W/m.K) |
0-100°C |
(n Ω .m) |
|
9.22 |
216 |
5.7 |
11.2 |
373 |
53.8 |



Hot Tags: uns n10629 pipe, China uns n10629 pipe suppliers, hastelloy metal pipe, alloy for batteries, alloy for condensers, Hastelloy Alloy S Seamless Pipe, Hastelloy C, nickel chromium molybdenum alloy