Hastelloy G3 Alloy Pipe
video

Hastelloy G3 Alloy Pipe

Hastelloy G3 alloy, referred to as G3, is a nickel-based corrosion-resistant alloy with superior performance. It belongs to the Ni-Cr-Fe system containing Mo and Cu. It has excellent resistance to oxidation, atmospheric corrosion and stress corrosion cracking, and has relatively good High resistance to local corrosion (pitting corrosion, crevice corrosion). Due to the high Fe content in the alloy, it has the characteristics of low cost compared with other nickel-based corrosion-resistant alloys. G3 alloy is commonly used in flue gas desulfurization systems, papermaking, and phosphoric acid production steam generators and heat exchangers. Oil well pipes made of this alloy have excellent resistance to H2S, CO2, and Cl- corrosion and are the best material for oil well pipes in sour gas fields. In the world, only Sumitomo of Japan, SMC of the United States, V&M of Germany and Sandvik of Sweden can produce it.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy g3 alloy pipe in China. If you're going to wholesale high quality hastelloy g3 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy G3 Alloy pipe

Product Introduction
Hastelloy G3 has good physical properties. The following are the general physical performance parameters of Hastelloy G3:

1. Density: The density of Hastelloy G3 is usually around 8.22 g/cm³ (0.297 lb/in³).

2. Melting point: The melting point of Hastelloy G3 is usually between 1399°C (2550°F) and 1427°C (2600°F).

3. Thermal expansion coefficient: The linear thermal expansion coefficient of Hastelloy G3 is usually around 13.9 μm/m·°C (7.7 μin/in·°F).

4. Thermal conductivity: The thermal conductivity of Hastelloy G3 is usually around 10.4 W/m·K (72.0 BTU·in/ft²·hr·°F).

5. Resistivity: The resistivity of Hastelloy G3 is usually around 1.28 μΩ·m (7.8 μΩ·in).

6. Magnetic: Hastelloy G3 is a non-magnetic material with good magnetic anti-interference performance.

Hastelloy G3 alloy, referred to as G3, is a nickel-based corrosion-resistant alloy with superior performance. It belongs to the Ni-Cr-Fe system containing Mo and Cu. It has excellent resistance to oxidation, atmospheric corrosion and stress corrosion cracking, and has relatively good

Hot Tags: hastelloy g3 alloy pipe, China hastelloy g3 alloy pipe suppliers, G 35 C 22HS Hastelloy Pipe, alloy for drawing, alloy for heat treatment, alloy for nuclear power plants, alloy for pumps, alloy for chemical industry

Send Inquiry

whatsapp

Phone

E-mail

Inquiry