Hastelloy C22 C276 Alloy SMLS Tubing
video

Hastelloy C22 C276 Alloy SMLS Tubing

Hastelloy 2.4602 Seamless Tube Dimensions
Length: 0.5 to 12 m
Wall Thickness: 0.5 to 30 mm
OD: 3 to 600 mm

Hastelloy C276 Seamless Tube
Dimensions: 4 - 219 mm
Wall Thickness: 0.5 - 20 mm
Lengths: Single, Double, Random Lengths and Cut to Length
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c22 c276 alloy smls tubing in China. If you're going to wholesale high quality hastelloy c22 c276 alloy smls tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy Pipe Products Application

hastelloy c22 c276 alloy ss tubing video

Hastelloy C22 Seamless Pipes Specification:

Specifications : ASTM B 622 ASME SB 622 / ASTM B 619 ASME SB 619
Dimensions : ASTM, ASME, and API
Size : 15″NB TO 150″NB IN
Specialized in : Large Diameter Size
Schedule : SCH5, SCH10, SCH40, STD, SCH80, SCH160
Type : Seamless / ERW / Welded / Fabricated
Form : Round, Hydraulic Etc
Length : Single Random, Double Random & Cut Length.
End : Plain End, Beveled End, Treaded

Specification List of Alloy C276 Seamless Tube

Specifications ASTM B 622 ASME SB 622 / ASTM B 619 ASME SB 619
Dimensions ASTM, ASME and API
Size 15″NB TO 150″NB IN
Specialized in Large Diameter Size
Schedule SCH5, SCH10, SCH40, STD, SCH80, SCH160
Type Seamless / ERW / Welded / Fabricated
Form Round, Hydraulic Etc
Length Single Random, Double Random & Cut Length.
End Plain End, Beveled End, Treaded

 

Hastelloy Material Specification

UNS N10276 Pipe Chemical Composition

Hastelloy C276 Ni C Mo Mn Si Fe P S Co Cr
Balance 0.010 max 15.00 – 17.00 1.00 max 0.08 max 4.00 – 7.00 0.04 max 0.03 max 2.5 max 14.50 – 16.50

C22 Hastelloy Alloy Pipes and Tubes Chemical Composition:

Hastelloy C22 Ni C Mo Mn Si Fe P S Co Cr
Balance 0.010 max 12.5 – 14.5 0.50 max 0.08 max 2 – 6 0.02 max 0.02 max 2.5 max 20 – 22.5

Hastelloy C22 Seamless Pipe Size

In. Sch Pipe
(mm)
C22 Pipe Kg/m
1/4 40S 2.23 13.72 0.64
1/2 10S 2.11 21.34 1.02
1/2 40S 2.77 21.34 1.29
3/8 80S 3.20 17.15 1.12
3/4 80S 3.91 26.66 2.23
1/2 80S 3.73 21.34 1.64
3/4 10S 2.12 26.68 1.30
3/4 40S 2.87 26.67 1.71
1/4 80S 3.02 13.72 0.81
3/8 10S 1.65 17.15 0.64
1/4 10S 1.64 13.72 0.50
3/8 40S 2.31 17.14 0.85
3/8 80S 3.20 17.15 1.12
1 10S 2.77 33.40 2.13
1 40S 3.37 33.40 2.54
1 80S 4.55 33.41 3.28
1 160 6.352 33.40 4.30
1¼ 10S 2.76 42.16 2.72
1¼ 40S 3.56 42.16 3.44

UNS N10276 Tubing Schedule Chart

1/8" IPS(.405"O. D.) 3 1/2" IPS( 4.000"O. D.)
SCH 40, 80 SCH 10, 40, 80, 160, XXH
1/4" IPS(.540"O. D.) 4" IPS(4.500"O. D.)
SCH 10, 40, 80 SCH 10, 40, 80, 160, XXH
3/8" IPS(.675"O. D.) 5" IPS( 5.563"O. D.)
SCH 10, 40, 80 SCH 10, 40, 80, 160, XXH
1/2" IPS(.840"O. D.) 6" IPS(6.625"O. D.)
SCH 5, 10, 40, 80, 160, XXH SCH 5, 10, 40, 80, 120, 160, XXH
3/4" IPS(1.050"O. D.) 8 " IPS(8.625"O. D.)
SCH 10, 40, 80, 160, XXH SCH 5, 10, 40, 80, 120, 160, XXH
1" IPS:(1.315′O. D.) 10" IPS(10.750"O. D.)
SCH 5, 10, 40, 80, 160, XXH SCH 10, 20, 40, 80 (.500), TRUE 80(.500)
1-1/4" IPS(1.660"O. D.) 12" IPS(12.750"O. D.)
SCH 10, 40, 80, 160, XXH SCH 10, 20, 40(.375), TRUE40(.406), SCH80(.500)
1-1/2" IPS(1.900"O. D.) 14" IPS(14.000"O. D.)
SCH 10, 40, 80, 160, XXH SCH10 (.188), SCH40 (.375)
2" IPS(2.375"O. D.) 16" IPS(16.000"O. D.)
SCH 10, 40, 80, 160, XXH SCH10(.188), SCH40(.375)
2 1/2" IPS(2.875"O. D.) 18" IPS (18.000"O. D.)
SCH 10, 40, 80, 160, XXH SCH-40 (.375)
3" IPS( 3.500"O. D.)  
SCH 5, 10, 40, 80, 160, XXH  

hastelloy c22 c276 alloy tubing

hastelloy c22 c276 tubing suppliersmaterial c22 c276 alloy tubing price

Hastelloy C-22 (UN S N06022/W.Nr. 2.4602/Alloy C-22) is a nickel-based high-temperature alloy containing nickel, molybdenum, cobalt, tungsten and other elements, with a nickel content of about 60%. It is a general-purpose nickel-chromium-molybdenum alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C-276, Alloy 625.Hastelloy C-22 alloy is a general-purpose nickel-chromium-molybdenum-tungsten alloy whose comprehensive properties are superior to other existing nickel-chromium-molybdenum alloys, including Hastelloy C-276, C4 alloy and 625 alloy.
C-276 Hastelloy is a nickel-molybdenum-chromium-iron-tungsten nickel-based alloy and is the most corrosion-resistant among modern metal materials. Mainly resistant to wet chlorine, various oxidizing chlorides, chloride salt solutions, sulfuric acid and oxidizing salts, and has good corrosion resistance in low and medium temperature hydrochloric acid. It is widely used in harsh corrosive environments, such as chemical industry, petrochemical industry, flue gas desulfurization, pulp and paper making, environmental protection and other industrial fields.

Products Description

C22 C276 Alloy SMLS Tubing

Hastelloy C22 C276 Alloy SMLS Tubing

Customer Case

customer visit

alloy c22 c276 tubing dealer

hastelloy c22 c276 piping stainless steel for sale

FAQ

 

 

 

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.

Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.

Q: About the product price of hastelloy c22 c276 alloy tubing?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

Hot Tags: Hastelloy C22 C276 Alloy SMLS Tubing, China Hastelloy C22 C276 Alloy SMLS Tubing suppliers, alloy for fuel cells, alloy for boilers, alloy for coating, alloy for catalytic converters, alloy for marine applications, alloy for forging

Send Inquiry

whatsapp

Phone

E-mail

Inquiry