Hastelloy X Flanges
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy x flanges in China. If you're going to wholesale high quality hastelloy x flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy X Flanges
Product Introduction
Hastelloy X flanges are excellent at forming and welding. While Alloy X is primarily known for its heat and oxidation resistance, these flanges also have good resistance to chloride stress corrosion cracking. Its corrosion resistance to SCC means these ASTM B564 UNS N06002 flanges are a very valuable asset in the petrochemical industry, where alloys need to combine high mechanical strength and corrosion resistance.
Hastelloy X Flanges Range
| Specification | ASTM B564 / ASME SB564 |
| Manufacturing Process | Hot Forging / Rolling / Machining |
| Outer Diameter | 1/2" NB TO 64" NB |
| Pressure Class | Class 150#, Class 300#, Class 400#, Class 600#, Class 900#, Class 1500#, Class 2500# or As Per Custom Requirement PN 6, PN 10, PN 16, PN 25 and PN 40 etc |
| Schedule | Sch 10s TO Sch XXS or As Per Custom Requirement |
| Facing | Flate Face (FF), Raised Face (RF), Ring Type Joint (RTJ) |
| Types | Welding Neck Flanges, Slip On Flanges, Socket Weld Flanges, Lap Joint Flange, Threaded Flange, Blind Flange, Orifice Flanges, Plate Flange, Long Welding Neck Flanges, Weldoflange, Nipoflange, Expander Flange, Reducing Flange, WNRF Flange, SORF Flange, SWRF Flange, Custom Flange as per Drawing etc. |
Composition Standard of Hastelloy Alloy X Flange
| Grade | Ni | Mo | Cr | Fe | Mn | C | Co | Si | P | S |
| Hastelloy X | Balance | 8.00 – 10.00 | 20.50 – 23.00 | 17.00 – 20.00 | 1.00 max | 0.05 – 0.15 | 0.50 – 2.50 | 1.00 max | 0.04 max | 0.03 max |
Mechanical Strength of X Hastelloy Flanges
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.22 g/cm | 1355°C | 655 MPa | 240 MPa | 35 |

Hot Tags: hastelloy x flanges, China hastelloy x flanges suppliers, alloy for annealing, material seamless piping, alloy for compressors, Hastelloy B, alloy for pumps, alloy for separators