Hastelloy C B-3 G-3 Alloy Pipe
video

Hastelloy C B-3 G-3 Alloy Pipe

Hastelloy C B-3 G-3 Pipe alloy belongs to NI-cr-mo alloy. It is mainly resistant to reducing medium and oxidizing medium corrosion.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c b-3 g-3 alloy pipe in China. If you're going to wholesale high quality hastelloy c b-3 g-3 alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy C B-3 G-3 Alloy Pipe

GNEE STEEL COMPANY

Our company is engaged in the production and trade of various alloy Hastelloy C B-3 G-3 tube, high-performance, high-precision special-shaped steel pipes and seamless pipes. We have established business relationships with customers in more than 20 countries and regions. Details such as payment method, delivery time and minimum quantity can be negotiated based on the order.

Ni……………..65 Min.
Mo……………28.5
Cr……………..1.5
Fe……………..1.5
W………………3 Max.
Mn……………..3 Max.
Co…..…………3 Max.
Al………………0.5 Max.
Ti……………….0.2 Max.
Si……………….0.1 Max.
C………………..0.01 Max.
V………………..0.2 Max.
Cu………………0.2 Max.
Ta……………….0.2 Max.
Zr……………….0.01 Max.

 

UNS Number N10276

W.Nr. 2.4819

Other common names: Alloy C276, Hastelloy C, Inconel® C-276

ASTM B574, B564, B575, B619, B626, B622

ASME SB574, SB564, SB575, SB619, SB626, SB622

Hot Tags: hastelloy c b-3 g-3 alloy pipe, China hastelloy c b-3 g-3 alloy pipe suppliers, B C4 Piping, alloy for extrusion, alloy for reactors, alloy for furnaces, hastelloy metal pipe, Hastelloy B2