Hastelloy C-276 Plates
video

Hastelloy C-276 Plates

Hastelloy C276 Plate Testing
Flanging Test
Microscopic and Macroscopic Tests
100% Radiographic Testing Report
Flattening Test
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c-276 plates in China. If you're going to wholesale high quality hastelloy c-276 plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy C-276 Plates description

 

Gnee Steel is a leading supplier of Hastelloy C276 steel plates in China and is ISO 9001:2015 certified. These steel plates are designed to withstand extreme conditions such as chemical processing, pollution control, and waste disposal. Made with nickel, molybdenum, and chromium, C276 steel plates offer excellent resistance to pitting, crevice corrosion, and stress corrosion cracking.

 

Hastelloy C276 Sheet & Plates

GNEE Hastelloy C-276 Plates

 

Hastelloy C276 sheet metal is designed to meet the extremely stringent Hastelloy C276 ASTM or ASME SB 575 standards and is considered a top-tier product for numerous applications. C276 sheet metal offers unparalleled reliability and durability even in the most demanding operating environments. The standard guarantees the sheet metal possesses the chemical composition, mechanical properties, and dimensions required for its intended use. Therefore, they are an ideal solution for businesses or academic institutions seeking reliable and durable engineering materials.

 

Gnee Steel manufactures Hastelloy C276 sheet metal in various sizes and thicknesses. We offer a wide range of options, including standard sizes and custom-sized cutting services. ASTM B575 UNS N10276 is favored by engineers and developers for its superior quality and durability. The price of C276 alloy sheet metal is influenced by factors such as market demand, alloy composition, and dimensions. However, given its excellent durability and low maintenance costs, investing in such high-quality material is undoubtedly a wise long-term decision. Nickel alloy C276 sheet metal is the preferred choice for professionals in many industries, especially for projects with extremely high corrosion resistance requirements. If you require Hastelloy C276 plates, coils, or strips, Gnee Steel is happy to provide you with a one-stop solution and top-notch products.

Hastelloy C276 Plate 

Hastelloy C276 Plate 

Hastelloy C276 Sheet 

Hastelloy C276 Sheet 

Hastelloy C276 Coil

Hastelloy C276 Coil 

 

Specification Of Hastelloy C-276 Plates

 

Specifications ASTM / ASME SB575
Size 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness 0.1mm to 12 mm Thk
Form Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

Hastelloy C-276 Plates Specification

 

Hastelloy C276 Sheet & Plates Equivalent Grades

STANDARD WERKSTOFF NR. UNS JIS GOST EN OR
Hastelloy C276 2.4819 N10276 NW 0276 ХН65МВУ NiMo16Cr15W ЭП760

 

Chemical Composition of Hastelloy Alloy C276 Sheet

Grade C Mn Si S Co Ni Cr Fe Mo P
Hastelloy C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4 – 7 15 – 17 0.04 max

 

Mechanical Properties of Hastelloy C276 Plates

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %

 

Thermal Properties of ASTM B575 Alloy C276 Plate

 

Properties Metric Imperial
Thermal expansion co-efficient (@24-93°C/75.2-199°F) 11.2 µm/m°C 6.22 µin/in°F
Thermal conductivity (-168 °C) 7.20 W/mK 50.0 BTU in/hr.ft².°F

 

Hastelloy C-276 Plates Dimension Data Sheet

 

Hastelloy C276 Plate Imperial Dimensions

Plate Surface finish Gauge (in) Width (max in)
2B – Cold rolled, heat treated, pickled, skin passed Plate 10–24 72*
2D – Cold rolled, heat treated, pickled plate 12–24 60
BA Mexinox only 18–28 48
Polished plate (not brushed) 11–24 60
Temper rolled plate Mexinox only 13–29 48

 

ASTM B127 Alloy C276 Plate Metric Dimensions

Plate Surface finish Thickness (mm) Width (max mm)
2B – Cold rolled, heat treated, pickled, skin passed plate 0.25–8.0 2032
2D – Cold rolled, heat treated, pickled plate 0.4–6.35 1524
2E – Cold rolled, heat treated, mechanically descaled plate 0.4–8.0 2032
2R – Cold rolled, bright annealed plate 0.25–3.5 1524
2H – Work hardened plate 0.4–6.35 1524
Polished, brushed plate 0.5–4.0 1524

 

Weight Chart of Hastelloy C-276 Plates

 

hickness Alloy Plate Weight per Unit Area Density
3/16 inches Hastelloy C276 0.06000 lbs/in²42.184176 kg/m² 0.315 lbs/in³8.72 g/cm³
1/4 inches Hastelloy C276 0.08 lbs/in²56.245568 kg/m² 0.315 lbs/in³8.72 g/cm³
3/8 inches Hastelloy C276 0.121 lbs/in²85.0714216 kg/m² 0.315 lbs/in³8.72 g/cm³
1/2 inches Hastelloy C276 0.161 lbs/in²113.1942056 kg/m² 0.315 lbs/in³8.72 g/cm³
5/8 inches Hastelloy C276 0.196 lbs/in²137.8016416 kg/m² 0.315 lbs/in³8.72 g/cm³
3/4 inches Hastelloy C276 0.235 lbs/in²165.221356 kg/m² 0.315 lbs/in³8.72 g/cm³
7/8 inches Hastelloy C276 0.274 lbs/in²192.6410704 kg/m² 0.315 lbs/in³8.72 g/cm³
1 inches Hastelloy C276 0.313 lbs/in²220.0607848 kg/m² 0.315 lbs/in³8.72 g/cm³
1 1/4 inches Hastelloy C276 0.391 lbs/in²274.9002136 kg/m² 0.315 lbs/in³8.72 g/cm³
1 1/2 inches Hastelloy C276 0.47 lbs/in²330.442712 kg/m² 0.315 lbs/in³8.72 g/cm³
1 3/4 inches Hastelloy C276 0.549 lbs/in²385.9852104 kg/m² 0.315 lbs/in³8.72 g/cm³
2 inches Hastelloy C276 0.627 lbs/in²440.8246392 kg/m² 0.315 lbs/in³8.72 g/cm³
2 1/4 inches Hastelloy C276 0.705 lbs/in²495.664068 kg/m² 0.315 lbs/in³8.72 g/cm³
2 1/2 inches Hastelloy C276 0.784 lbs/in²551.2065664 kg/m² 0.315 lbs/in³8.72 g/cm³
2 3/4 inches Hastelloy C276 0.862 lbs/in²606.0459952 kg/m² 0.315 lbs/in³8.72 g/cm³
3 inches Hastelloy C276 0.941 lbs/in²661.5884936 kg/m² 0.315 lbs/in³8.72 g/cm³

 

Hastelloy C276 boards are in stock and can be shipped immediately to meet urgent needs.

 

Customized Hastelloy C276 0.6mm Plate for Heat Exchanger Plate

Custom Hastelloy C276 0.6mm heat exchange plate

Hot Rolled Hastelloy C276 8mm 10mm 12mm Sheet

Hot-rolled Hastelloy C276 plates in 8mm, 10mm, and 12mm thicknesses

1-5mm Hastelloy C276 Nickle Alloy Steel Plate

1-5mm Hastelloy C276 Nickle Alloy Steel Plate

AMS 5607 Industry Equipment Hastelloy C276 Nickel Alloy Plate

AMS 5607 Industry Equipment Hastelloy C276 Nickel Alloy Plate

Corrosion Resistant Bright Hastelloy C276 Sheet

Corrosion Resistant Bright Hastelloy C276 Sheet

1mm 6mm Nickel Based Hastelloy C276 Sheet

1mm 6mm Nickel Based Hastelloy C276 Sheet

 

Hastelloy C276 B575 N10276 Plate and Sheet Prices

 

Description Price Range in USD  
Nickel Alloy C276 Plate / Sheet Price $25.00 - $35.00 per Kilogram  
Price for Nickel Alloy C276 Plate / Sheet $35.00 - $38.00 per Kilogram  
Hastelloy C276 Alloy Plate 4 x 8 ft $3,000.00 - $3,800.00 per Ton  
ASME SB575 Hastelloy C276 Plate 3mm thickness $20.00 - $70.00 per Kilogram  
Nickel Alloy 2.4819 Plate/Sheet Price Per Kg $20.00 - $40.00 per Kilogram  
ASTM B575 N10276 Hastelloy Alloy Plate $50.00 per Kilogram  
Nickel Base Alloy C276 Clad Plate $31.77 - $37.77 per Kilogram  
UNS N10276 Alloy Plate Sheet $20.00 - $35.00 per Kilogram  

 

Hastelloy C-276 Plates Application

 

Hastelloy C-276 Plates Application

Hastelloy C-276 Plates Application

 

 

About Gnee Steel

 

product-875-492

 

About Gnee Steel

Request the latest Hastelloy C-276 Plate price list. Please call +8615824687445 or email ss@gneesteel.com for information on available stock and the latest price list for Hastelloy C-276 Plate.

 

FAQ

Q: How difficult is it to machine Hastelloy C276 sheet?

A: Medium to difficult

Q: What is the cutting speed for hot-rolled Hastelloy C276 sheet?

A: 50 m/min

Q: What is the corrosion rate of Hastelloy C276 sheet?

A: 6.47 ± 0.20 mm/year

Hot Tags: hastelloy c-276 plates, China hastelloy c-276 plates suppliers, alloy for turning, alloy for nuclear power plants, Hastelloy Alloy C22 Round Bars, UNS N06455 N10629 Hastelloy Pipe, alloy for piping systems, alloy for normalizing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry