Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy alloy c 2000 in China. If you're going to wholesale high quality hastelloy alloy c 2000 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Hastelloy Alloy C 2000
The following table shows the chemical composition of Hastelloy(r) C-2000(r).
|
Element |
Content (%) |
|
Nickel, Ni |
59 |
|
Chromium, Cr |
23 |
|
Molybdenum, Mo |
16 |
|
Copper, Cu |
1.6 |
|
Silicon, Si |
0.080 |
|
Carbon, C |
0.010 |
Application
Hastelloy(r) C-2000(r) can be used in applications requiring high metallurgical stability in reducing or oxidizing atmospheres. It is also used in chemical process equipment applications.
Feature
Hastelloy C-2000 has the following key properties:
Specifically developed to resist corrosion in a wider range of media.
Resists a wide range of corrosive chemicals, including sulfuric acid, hydrochloric acid and hydrofluoric acid.
Excellent pitting and crevice corrosion resistance compared to Hastelloy C-276.
Excellent corrosion resistance to reducing media.
Good antioxidant properties.