C-22HS G-35 Hastelloy Metal Pipe And Tube
video

C-22HS G-35 Hastelloy Metal Pipe And Tube

C-2HS is a multifunctional nickel complex alloy. It is a high-strength version of (22 alloy). It has excellent oxidation and reduction capabilities and can obtain high strength through heat treatment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c-22hs g-35 hastelloy metal pipe and tube in China. If you're going to wholesale high quality c-22hs g-35 hastelloy metal pipe and tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

C-22HS G-35 Hastelloy Metal Pipe

C-22HS G-35 Hastelloy Metal Pipe Specification

 

Grade

C

Mn

Si

S

Co

Ni

Cr

Fe

Mo

P

Alloy C22

0.010 max

0.50 max

0.08 max

0.02 max

2.50 max

50.015 min*

20.00 – 22.50

2.00 – 6.00

12.50 – 14.50

0.02 max

 

C-22HSG-35 Hastelloy Metal PipeC-22HSG-35 Hastelloy Metal Pipe

 