SS Plate ASME SA240 S32205 , S31803 Duplex Steel 2205 Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss plate asme sa240 s32205 , s31803 duplex steel 2205 plate in China. If you're going to wholesale high quality ss plate asme sa240 s32205 , s31803 duplex steel 2205 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Applications
Pressure vessels, tanks, piping, and heat exchangers in the chemical processing industry
Piping, tubing, and heat exchangers for the handling of gas and oil
Effluent scrubbing systems
Pulp and paper industry digesters, bleaching equipment, and stock-handling systems
Rotors, fans, shafts, and press rolls requiring combined strength and corrosion resistance
Cargo tanks for ships and trucks
Food processing equipment
Biofuels plants
Mechanical Properties at Room Temperature
|
|
ASTM A 240 |
Typical |
|
Yield Strength 0.2%, ksi |
65 min. |
74 |
|
Tensile Strength, ksi |
90 min. |
105 |
|
Elongation % |
25 min. |
30 |
|
Hardness HB |
293 max. |
256 |
Physical Properties
|
Temperature °F |
|
68 |
212 |
392 |
572 |
|
Density |
lb/in3 |
0.278 |
-- |
-- |
-- |
|
Modulus of Elasticity |
psi x 106 |
27.6 |
26.1 |
25.4 |
24.9 |
|
Linear Expansion (681T4F-T) |
10-6/°F |
-- |
7.5 |
7.8 |
8.1 |
|
Thermal Conductivity |
Btu/h ft. °F |
8.7 |
9.2 |
9.8 |
10.4 |
|
Heat Capacity |
Btu/lb/°F |
0.112 |
0.119 |
0.127 |
0.134 |
|
Electrical Resistivity |
in x 10-6 |
33.5 |
35.4 |
37.4 |
39.4 |
Hot Forming
Forming below 600°F is recommended whenever possible. When hot forming is required, the workpiece should be heated uniformly and worked in the range of 1750 to 2250°F. Alloy 2205 is quite soft at these temperatures and is readily formed. Above this range, 2205 is subject to hot tearing. Immediately below this range, the austenite becomes substantially stronger than the ferrite and may cause cracking, a particular danger to "cold" edges. Below 1700°F there can be rapid formation of intermetallic phases because of the combination of temperature and deformation. Whenever hot forming is done, it should be followed by a full solution anneal at 1900°F minimum and rapid quench to restore phase balance, toughness, and corrosion resistance. Stress relieving is not required or recommended; however, if it must be performed, the material should receive a full solution anneal at 1900°F minimum, followed by rapid cooling or water quenching.




FAQ
Q: Can provide OEM/ODM service?
A: Yes. Please feel free to contact us for more details discuss.
Q: How is your Payment Term?
A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.
Q: Can I get samples before order ?
A: Yes, of course.We can produce by your samples or technical drawings ;
Q: Can I go to your factory to visit?
A: Of course, we welcome customers from all over the world to visit our factory ;
Q:What are the shipping ports?
A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Hot Tags: ss plate asme sa240 s32205 , s31803 duplex steel 2205 plate, China ss plate asme sa240 s32205 , s31803 duplex steel 2205 plate suppliers, duplex stainless steel thickness, duplex stainless steel packaging, duplex stainless steel standard, duplex stainless steel strip, duplex stainless steel wholesaler, duplex stainless steel weight
You Might Also Like
Send Inquiry