AISI 420 Sheet TISCO 20Cr13 SUS420J1Stainless Steel Plate
video

AISI 420 Sheet TISCO 20Cr13 SUS420J1Stainless Steel Plate

AISI 420 stainless steel (SS420) is a straight chromium martensitic stainless steel grade with certain wear resistance, corrosion resistance and high hardness.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of aisi 420 sheet tisco 20cr13 sus420j1stainless steel plate in China. If you're going to wholesale high quality aisi 420 sheet tisco 20cr13 sus420j1stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

AISI 420 stainless steel (SS420) is a straight chromium martensitic stainless steel grade with certain wear resistance, corrosion resistance and high hardness.

SS 420 stainless steel physical properties are listed in the table below such as density, melting point, specific heat, electrical resistivity, elastic modulus, thermal conductivity, and coefficient of thermal expansion (CTE).

Datasheet 2, 420 stainless steel properties – 1.

SS 420 Physical Properties
Density, g/cm3 (lb/in.3) 7.8 (0.28)
Melting point, °C (°F) 1450-1510 (2650-2750)
Specific heat capacity, J/kg·K (Btu/lb·°F) 460 (0.11) at 0-100 °C (32 to 212 °F)
Electrical resistivity, μΩ·m 0.55 at 20 °C
Elastic modulus (Modulus of elasticity), GPa (106 psi) 200 (29)
Thermal conductivity, W/m·K (Btu/ft·h·°F) 24.9 (14.4), at 100 °C (212 °F)
Coefficient of thermal expansion, μm/m·°C (μin./in. ·°F) 10.3 (5.7), at 0-100 °C (32-212 °F)
10.8 (6.0), at 0-315 °C (32-600 °F)
11.7 (6.5), at 0-538 °C (32-1000 °F)

 

Type 420 stainless steel heat treatment includes annealing, hardening, tempering and stress relief. Preparation for heat treatment includes precleaning, preheating, atmosphere protection, salt bath, and hydrogen embrittlement.

Precleaning: All workpieces of SS420 and fixtures must be thoroughly cleaned, such as oil, sweat and other stains on the surface of the workpiece.Preheating: The thermal conductivity of type 420 stainless steel is usually lower than that of carbon steel. When heating rapidly, the workpiece is easily deformed and cracked. Therefore, preheating is recommended. The preheating temperature is generally 760-790 °C (1400-1450 °F). Heavy-duty parts can be preheated in two stages: Preheat at 540 °C (1000 °F) firstly, and then heat to 790 °C (1450 °F).Atmosphere protection: Austenitizing temperature 1010 °C (1850 °F), dew-point temperature: 10-12 °C (50-54 °F) for AISI 420 wrought martensitic stainless steel.Salt bath: Bath salts give 420 grade stainless steel (SS 420) parts a better result.Hydrogen embrittlement: Hydrogen embrittlement is a serious problem with 420 steel.

321 Stainless Steel Medium Thick Plate321 Stainless Steel Medium Thick Plate

 

product-369-360product-800-800

FAQ

Q: Can provide OEM/ODM service?

A: Yes. Please feel free to contact us for more details discuss.

Q: How is your Payment Term?

A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Hot Tags: aisi 420 sheet tisco 20cr13 sus420j1stainless steel plate, China aisi 420 sheet tisco 20cr13 sus420j1stainless steel plate suppliers, duplex stainless steel corrosion resistance, duplex stainless steel alloy, duplex stainless steel alkali resistance, duplex stainless steel wear resistance, duplex stainless steel scalability, duplex stainless steel development

Send Inquiry

whatsapp

Phone

E-mail

Inquiry