ASTM A182 F51 Duplex 2205 Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a182 f51 duplex 2205 round bar in China. If you're going to wholesale high quality astm a182 f51 duplex 2205 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
The standard specification of the F51 round bar is Duplex 2205. Other equivalents are UNS S 31803 and Werkstoff Nr. 1.4462. It consists of chromium, nickel, iron, manganese, molybdenum, and carbon. The material's tensile strength and resistance to stress-cracking corrosion are outstanding. Hence, they're widely popular in the petrochemical, desalination, oil, and gas industries.
The density of the A182 gr F51 flat bar is 7.8 g/cm3 at 20 degrees Celsius. Its chemical composition is 21% to 23% Chromium, 4.5% to 6.5% Nickel, 2.5% to 3.5% Molybdenum, 2% Manganese, 1% Silicon, 0.8% to 2% Nitrogen, 0.03% Phosphorus, 0.03% Carbon, and 0.02% Sulfur. The material's yield strength is 450 MPa and its tensile strength is 620 MPa. Its elongation is 25%.Yes, ASTM A479 S31803 bright bar can be polished. The polishing of the material usually happens with a bright bar polishing machine or belt polishing machine. Electropolishing of the bright bars is also possible and it also increases the corrosion resistance.The bright bars have a great precision and surface finish that is useful in various industries. The various surface finishes of duplex bars are bright black finish, smooth, turned, centerless grounded, forged rough, etc.The tolerances of cold-drawn UNS S31803 round bar for sizes between 6 mm to 400 mm ranges from 0.07 mm to 0.25 mm. You can multiply both the diameters of the cold-drawn bars with 0.00623 to get its weight per meter. When you multiply the diameters of the bar with 0.0019, you will get its weight per foot.




FAQ
Q: Can I get samples before order ?
A: Yes, of course.We can produce by your samples or technical drawings ;
Q: Can I go to your factory to visit?
A: Of course, we welcome customers from all over the world to visit our factory ;
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Hot Tags: astm a182 f51 duplex 2205 round bar, China astm a182 f51 duplex 2205 round bar suppliers, duplex stainless steel improvement, duplex stainless steel replacement, duplex stainless steel corrosion resistance, duplex stainless steel durability, duplex stainless steel packaging, duplex stainless steel use