Seel Plate Laser Cutting F55 Super Duplex
video

Seel Plate Laser Cutting F55 Super Duplex

S32760, also called F55 or 1.4501, is a high-alloy super duplex stainless steel, featuring strong strength and corrosion resistance, mainly used in a variety of strong corrosion environments such as chemical processing, petrochemical and submarine equipment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of seel plate laser cutting f55 super duplex in China. If you're going to wholesale high quality seel plate laser cutting f55 super duplex made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Just like other super duplex stainless steels, S32760 stainless steel microstructure presents a two-phase structure with α/γ close to 1 under solid solution conditions. However, undergoing from high temperature to room temperature like incorrect thermal processing, heat treatment and welding process, during which cooling processes, there will be intermetallic phases and nitrides on the substrate of S32760 stainless steel. When exposed to temperature at around 900 °C for more than 100 seconds, σ, χ, Cr2N, etc. will precipitate on the substrate; at about 475 °C for more than 800 seconds, the α phase will precipitate. In order to avoid the precipitation of the intermetallic phase and the Cr2N phase, it must have a sufficient cooling rate during the cooling process. Plus, this super duplex stainless steel does not adapt to heat treatment and cooling to produce σ phase.

S32760 Applications

1) Neutral chloride environment;

2) Oil refining industry;

3) Pipeline used for chemical industry;

4) Oil and gas industry;

5) Pulp and paper industry;

6) Fertilizer industry, urea industry, phosphate fertilizer industry;

7) Seawater environment, energy and environmental protection industry;

8) Light industry and food industry, food and pharmaceutical industry equipment;

9) High strength structural parts;

10) Hood desulfurization, infiltration desalination equipment, sulfuric acid plant;

11) Submarine pipelines, marine engineering fasteners, etc.;

12) Others.

Chemical composition for S32506 Stainless steel (Max%)

Main chemical elements composition of A240 S32506
C Si Mn P S Cr
0.030 0.90 1.00 0.040 0.015 24.0-26.0
Ni Mo N      
5.5-7.2 3.0-3.5 0.08-0.20      

product-317-313product-600-450product-818-614product-800-800

 

FAQ

Q: Can I get your best price?

A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Q: Why choose us?

A: We are an iron and steel enterprise integrating industry and trade, Our company have been in steel business for more than ten years, we are internationally experienced, professional, and we can provide variety of steel products with high quality to our clients.

Hot Tags: seel plate laser cutting f55 super duplex, China seel plate laser cutting f55 super duplex suppliers, duplex stainless steel quotation, duplex stainless steel part, duplex stainless steel transportation, duplex stainless steel stock, duplex stainless steel reducer, duplex stainless steel integration

Send Inquiry

whatsapp

Phone

E-mail

Inquiry