S32760 Stainless Steel Plate F55 Super Duplex Seel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s32760 stainless steel plate f55 super duplex seel plate in China. If you're going to wholesale high quality s32760 stainless steel plate f55 super duplex seel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
S32760 duplex steel also features strong resistance to chloride corrosion, high thermal conductivity and low coefficient of thermal expansion. Higher chromium, molybdenum and nitrogen content make it highly resistant to pitting, crevice corrosion and other corrosions. The excellent overall performance of S32760 duplex steel is superior to that of general dual phase steel, such as 2205, S31803 and so on.S32760 duplex steel is resistant to various inorganic acids and organic acids. The copper added makes it resistant to non-oxidative acid corrosion. S32760 is also resistant to strong alkali corrosion, but it is not suitable to work at temperatures above 300 ° C for a long time, because a long-term exposure to such high temperature will lead to reduced toughness of the material.
S32760 stainless steel was used as cast steel in the early 1980s to make up the insufficient corrosion resistance of the second-generation duplex stainless steel 00Cr22Ni5Mo2N (2205). In the late 1980s, it came to be used as the deformable material for pipeline systems. Subsequently, this super duplex was introduced as an important corrosion-resistant material into oil and gas development, seawater environment, flue gas desulfurization (FGD), desalination, and chemical applications.
S32760 stainless steel also contains a small amount of tungsten and copper in addition to high chromium, molybdenum and nitrogen. In early times, tungsten and copper were added to improve the casting properties of this alloy. Later, it was found that tungsten and copper could enhance the corrosion resistance of the steel in certain acids and its ability to passivate in seawater.




FAQ
Q: Can I get your best price?
A: Our goal is to provide you the best price with great quality assured in a long run. Please leave your contact information for the best quotations, we will get back to you with the best solutions as soon as we can.
Q:What are the shipping ports?
A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Q: Why choose us?
A: We are an iron and steel enterprise integrating industry and trade, Our company have been in steel business for more than ten years, we are internationally experienced, professional, and we can provide variety of steel products with high quality to our clients.
Hot Tags: s32760 stainless steel plate f55 super duplex seel plate, China s32760 stainless steel plate f55 super duplex seel plate suppliers, duplex stainless steel durability, duplex stainless steel user, duplex stainless steel warranty, duplex stainless steel market, duplex stainless steel processing, duplex stainless steel wire
You Might Also Like
Send Inquiry