254 Smo Round Bar UNS S31254
video

254 Smo Round Bar UNS S31254

The duplex steel rod has a microstructure of two phases- Ferritic and Austenitic. The composition of Duplex steel has more Chromium and Molybdenum. The above properties make the alloy highly resistant to corrosive environments, especially salt water. Hence, they are popularly applicable in desalination systems, pipes, and pumps with saltwater exposure.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 254 smo round bar uns s31254 in China. If you're going to wholesale high quality 254 smo round bar uns s31254 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SMO254 is a combination of chromium, nitrogen, Molybdenum, and nitrogen. It has excellent corrosion resistance and so is used in chloride-containing environments and against sulphuric acid. 254 smo stainless steel rounds have high strength compared to SS316.

SS 316 round bar has nickel, chromium, and molybdenum which gives high corrosion resistance and strength to the material. The material is easily weldable and machinable.

The equivalents for smo 254 flat bar are:

Werkstoff 1.4547

UNS S31254

SIS 2378.

The manufacturing process of the material includes,

The bending of the material ranges between cold bending and tight bending.

Machining of the material with reduced cutting speed.

Heat Treatment with Solution annealing between 1150°C to 1200°C.

The composition of smo 254 alloy is Iron, Nickel, Chromium, Molybdenum, Nitrogen, and Carbon. There are several inspection methods for alloy 254 bright bars; they are:

Raw Material Testing

Corrosion Resistance Test

Hardness Test

Flaring Test

Tensile Testing

Heat Treatment Documents

Fumigation Tests

Quality Assurance Certificates

Metallography

Ultrasonography

Corrosion-resistant 254SMO stainless steel bar, 254SMO stainless steel round bar.
254SMO stainless steel round bar (round bar) belongs to the category of long products, and also belongs to the category of 254SMO bars. 254SMO stainless steel bright bar: the surface is smooth and is processed by quasi-rolling; while 254SMO black bar refers to the surface is black and rough and is directly hot-rolled. 254SMO stainless steel bar specifications:
Material: 303, 303F, 304, 304F, 304L, 321, 314, 316, 316L, 316F, 310S, 630, 904L, 254SMO, 416F, 1Cr13, 2Cr13, 3Cr13, 1Cr17Ni2, duplex steel, antibacterial steel and other materials! [1] Application range: petroleum, electronics, chemical, medicine, textile, food, machinery, construction, nuclear power, aerospace, military industry and other industries.

product-536-536product-1920-2560

product-1000-1000product-405-228

FAQ

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q: What are the advantages of your company ?

A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Hot Tags: 254 smo round bar uns s31254, China 254 smo round bar uns s31254 suppliers, duplex stainless steel modification, duplex stainless steel availability, duplex stainless steel maintainer, duplex stainless steel pressure resistance, duplex stainless steel research, duplex stainless steel upgrade

Send Inquiry

whatsapp

Phone

E-mail

Inquiry