LDX 2101 Duplex Stainless Steel Round Bar
video

LDX 2101 Duplex Stainless Steel Round Bar

A Lean Duplex Round Bar is designed possessing a uniform cross-sectional area. These bars are very versatile and have good adaptability in different conditions. The LDX 2101 SS Round Bar provides strength and stability to a wide spectrum of applications in extreme conditions as it has a higher melting point.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ldx 2101 duplex stainless steel round bar in China. If you're going to wholesale high quality ldx 2101 duplex stainless steel round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

LDX 2101 Duplex Stainless Steel Round Bar Description

LDX 2101 Duplex Stainless Steel Round Bar

GNEE STEEL GROUP supplies LDX 2101 Duplex Stainless Steel Round Bar for you

A Lean Duplex Round Bar is designed possessing a uniform cross-sectional area. These bars are very versatile and have good adaptability in different conditions. The LDX 2101 Round Bar provides strength and stability to a wide spectrum of applications in extreme conditions as it has a higher melting point. An LDX 2404 Round Bar has good abrasion, erosion, and fatigue resistance. These bars can be readily welded following standard welding procedures. They have good energy absorption and low thermal expansion. The 1.4362 Stainless Steel Bar has resistance to stress-corrosion cracking and showcases outstanding tensile and yield strength. These bars have uniform resistances and tolerances throughout the fixture.

 

GNEE LDX 2101 round rod specifications

Specifications: ASTM, ASME and API

Standard specifications: ASTM A276, A479 / ASME SA276, SA479

Dimensions: diameter 10mm to 100mm, length 100mm to 6000mm.

Length: 3 to 6 meters, custom cut to length

Surface treatment: black, bright polished, rough turning, NO.4 surface treatment, matte surface treatment, BA surface treatment

Our UNS S32101 LDX 2101 Round Bar complies with NACE MR0175/ISO 15156

 

Available Product Types AISI, ASME, ASTM, DIN, Duplex Steel S32101 LDX 2101 Round Bar

Duplex Steel LDX 2101 Rod
Duplex steel UNS S32101 LDX 2101 round steel
ASTM A479 UNS S32101 LDX 2101 Bar
ASTM A276 Dual Phase Steel UNS S32101 LDX 2101 Round Bar
ASTM A276 Dual Phase Steel UNS S32101 LDX 2101 Rod Manufacturer
LDX 2101 Duplex Steel Polishing Rod Manufacturer
AISI Duplex Steel UNS S32101 LDX 2101 Black Rod Distributor
Premium Duplex Steel LDX 2101 Spring Steel Rod
ASTM A479 UNS S32101 LDX 2101 Duplex Steel Bright Rod Exporters
UNS S32101 LDX 2101 forged round steel

The largest inventory of duplex steel LDX 2101 threaded bars in China
Duplex Steel LDX 2101 Cold Drawn and Polished Square Steel
Austenitic ASTM Dual Phase Steel LDX 2101 Bright Bar
Duplex steel F60 WERKSTOFF NR. 1.4162 round steel
Duplex Steel UNS S32101 LDX 2101 Hexagonal Rod Dealer
Duplex Steel LDX 2101 Cold Drawn Bar
High Speed ​​Steel LDX 2101 Duplex Steel Hollow Rod Supplier
ASME, ASTM, DIN LDX 2101 Duplex Steel Flat Steel
AISI ASTM Dual Phase Steel UNS S32101 LDX 2101 Round Steel
Cold rolled dual phase steel UNS S32101 LDX 2101 Hot forged bar

LDX 2101 Duplex Stainless Steel Round Bar Properties


LDX 2101 Duplex Stainless Steel Round Bar Chemical Composition

  Ni Cr Mo Mn Cu Si C N S P Fe
MIN 1.35 21.0 0.1 4.0 0.1 - - 0.2 - - -
MAX 1.7 22.0 0.8 6.0 0.8 1.0 0.04 0.25 0.03 0.04 Balance


Alloy LDX 2101 Round Bar Sizes

1/4" 3/16" 5/16" 1/2" 3/8" 5/8" 3/4"
6.3mm 4.8mm 7.9mm 12.7mm 9.5mm 15.9mm 19mm
1" 7/8" 1 1/4" 1 3/4" 1 1/2" 2"  
25.4mm 22.2mm 31.8mm 44.5mm 38.1mm 50.8mm  

 LDX 2101 Duplex Stainless Steel Round Bar PropertiesLDX 2101 ss  Round Bar

Duplex stainless steels are extremely corrosion resistant, work hardenable alloys. Their microstructures consist of a mixture of austenite and ferrite phases. As a result, duplex stainless steels display properties characteristic of both austenitic and ferritic stainless steels. Duplex stainless steels are in most cases, tougher than ferritic stainless steels. Strengths of duplex stainless steels can in some cases be double that for austenitic stainless steels.Whilst duplex stainless steels are considered resistant to stress corrosion cracking, they are not as resistant to this form of attack as ferritic stainless steels. However, the corrosion resistance of the least resistant duplex stainless steels is greater than that for the most commonly used grades of stainless steels, i.e. 304 and 316.Duplex steels are also magnetic, a property that can be used to easily differentiate them from common austenitic grades of stainless.

 

Customer Case

gnee steel Customer Case

LDX 2101 Duplex Stainless Steel Round Bar

About US

 

 Rich Experience

GNEE Steel Group was founded in 2008 and has more than 10 years of experience in manufacturing steel.

 

 One-Stop Solution

GNEE Steel Group is a professional, one-stop supply chain enterprise for steel products, covering product research and development, sales, promotion, and providing professional services.

 

 Broad Market

The company's products are sold to Europe, Australia, and exported to more than 70 countries around the world. It has a total of more than 800 global cooperative enterprises, which include 15 shipbuilding companies, 143 engineering project companies, and 23 boiler machinery manufacturers.

 

 Delivery on Time

Our annual product sales volume is 1 million tons, our inventory is 200,000 tons, and our annual export volume has reached 80,000 tons, ensuring on-time delivery.

 

FAQ

 

Q: How can I get a quotation from you ?
A:You can leave us message, and we will reply every message in time. Or we may talk on line by Trademanager.
Q:Can I get samples before order ?
A:Yes, of course. Usually our samples are free. we can produce by your samples or technical drawings. We can build the molds and fixtures.
Q:How can you garantee what I got will be good ?
A:We are factory with 100% predelivery inspection which garantee the quality.And as golden supplier on Alibaba. Alibaba assurance will make garantee,which means alibaba will pay your money back in advance if there is any problem with the products.

Q: What product information must I provide before purchasing?
A:Please provide the grade, width, thickness, surface treatment requirements and the quantity you require.
Q: What shipping ports are there?
A:We usually ship from Shanghai, Tianjin, Qingdao and Ningbo ports.

Q: About the product price of LDX 2101 Duplex Stainless Steel Round Bar?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: ldx 2101 duplex stainless steel round bar, China ldx 2101 duplex stainless steel round bar suppliers, duplex stainless steel research, duplex stainless steel width, duplex stainless steel identification, duplex stainless steel construction, duplex stainless steel sell, duplex stainless steel substitute

Send Inquiry

whatsapp

Phone

E-mail

Inquiry