Duplex Stainless Steel Bars F60 and UNS S32707 are a highly reliable and versatile product in the stainless steel industry. They are characterized by their excellent strength, excellent corrosion resistance and excellent toughness, making them ideal for use in environments demanding high performance.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of duplex stainless steel bars f60 and uns s32707 in China. If you're going to wholesale high quality duplex stainless steel bars f60 and uns s32707 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Duplex Stainless Steel Bars F60 and UNS S32707 are a highly reliable and versatile product in the stainless steel industry. They are characterized by their excellent strength, excellent corrosion resistance and excellent toughness, making them ideal for use in environments demanding high performance.

1029 30

F60 and UNS S32707 are both dual-phase stainless steel grades, which contain both austenitic and ferritic phases in their microstructure. The combination of these two phases makes for an exceptionally strong and robust steel that is resistant to corrosion, crevice corrosion, stress corrosion cracking and erosion.

 

These duplex stainless steel bars offer high resistance to several chemicals, including acids, alkalis, and chlorides. They are particularly useful in environments with high chloride ion concentration or acidic conditions. Moreover, their unique combination of high strength and excellent toughness makes duplex stainless steel bars suitable for use in high-pressure applications such as oil and gas exploration and production.

 

Type of Bar F60 UNS S32707
Diameter (mm) 6-250 6-250
Length (mm) 1000-6000 1000-6000
Surface Finish Black, bright, peeled, ground or polished Black, bright, peeled, ground or polished
Standard ASTM A276, A479, A484 ASTM A276, A479, A484
Chemical Composition C≤0.03; Si≤1.00; Mn≤2.00; P≤0.035; S≤0.020; Cr=25.0-26.5; Ni=6.0-8.0; Mo=3.0-4.0; N=0.20-0.30 C≤0.030; Si≤1.00; Mn≤2.00; P≤0.035; S≤0.020; Cr=26.0-29.0; Ni=6.0-8.0; Mo=3.5-5.5; N=0.20-0.35
Mechanical Properties Tensile Strength (MPa)≥630; Yield Strength (MPa)≥450; Elongation (%)≥25; Hardness (HB)≤290 Tensile Strength (MPa)≥750; Yield Strength (MPa)≥550; Elongation (%)≥15; Hardness (HB)≤290

277

In addition, these duplex stainless steel bars require minimal maintenance, which makes them a preferred choice for use in marine and offshore applications. They are also easy to fabricate and weld, making them an ideal choice for a wide range of applications in various industries, including construction, chemical processing, nuclear power plants, and food and beverage processing.

 

Overall, F60 and UNS S32707 duplex stainless steel bars are a reliable, high-performance, and cost-effective solution for demanding applications requiring exceptional strength, excellent corrosion resistance, and excellent toughness. They are an excellent choice for anyone looking for a reliable and versatile product that will provide long-term service and excellent value for money.

 

Hot Tags: duplex stainless steel bars f60 and uns s32707, China duplex stainless steel bars f60 and uns s32707 suppliers, duplex stainless steel resource efficiency, duplex stainless steel substitute, duplex stainless steel vessel, duplex stainless steel recyclability, duplex stainless steel distributor, duplex stainless steel warranty