ZR 704 ZR 702 Zirconium Alloy Tubes
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of zr 704 zr 702 zirconium alloy tubes in China. If you're going to wholesale high quality zr 704 zr 702 zirconium alloy tubes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Zirconium Products Application
ZR 704 Zirconium Alloy Tubes video
Zirconium 702 tubing is resistant to most organic and inorganic acids. Typical applications for seamless zirconium tubes are heat exchangers, coolers, condensers and piping systems in the production of urea, acetic acid, formic acid, nitric acid and methyl methacrylate.
Zirconium Material Specification
|
Grade |
Zr702 (R60702) |
Zr704 (R60704) |
Zr705 (R60705) |
|
Zr+Hf |
99.20% |
97.50% |
95.50% |
|
Hf |
<4.5% |
<4.5% |
<4.5% |
|
Fe+Cr |
<0.20% |
0.2-0.4% |
<0.2% |
|
Sn |
- |
1.0-2.0% |
- |
|
H |
<0.005% |
<0.005% |
<0.005% |
|
N |
<0.015% |
<0.015% |
<0.015% |
|
C |
<0.030% |
<0.030% |
<0.050% |
|
O |
<0.15% |
<0.16% |
<0.16% |
|
Nb |
- |
- |
2.0-3.0% |


Zirconium alloy wire (Zr 704) has excellent resistance to highly corrosive environments (such as high-concentration acid and alkali solutions). GNEE Steel has extensive experience in manufacturing and supplying high quality Zirconium Alloy Wire (Zr 704).
Zirconium alloy wire (Zr 704) is a tin-containing zirconium alloy. It has excellent resistance to highly corrosive environments such as high-concentration acids and alkaline solutions.
Zr702 "Zirconium Alloy" is a high-performance alloy material composed of zirconium as the main element. Zirconium alloy has excellent mechanical properties, corrosion resistance and thermal stability, so it is widely used in aerospace, shipbuilding, chemical industry, and nuclear industry and other fields.
Customer Case
customer visit


FAQ
Q:How to pack the products?
A:The inner layer has a waterproof paper outer layer with iron packaging and is fixed with a fumigation wooden pallet. It can effectively protect products from corrosion during ocean transportation.
Q:What is your working time?
A:In general, our online service time is time: 9:00-22:00, after 22:00, we will reply to your inquiry during the next working day.
Q: What are your company's strengths?
A:Factory spot, competitive prices, excellent quality, support factory inspection, video call at any time, technical support.Simultaneously, we have participated in many international projects.
Q: What trade terms do you usually use?
A: We use FOB, CIF, EXW,FCA,FAS,CFR.
Q: What are your terms of payment?
A: We use TT and LC, or any other payment method available.
Q: About the product price of ZR 704 Zirconium Alloy Tubes?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: zr 704 zr 702 zirconium alloy tubes, China zr 704 zr 702 zirconium alloy tubes suppliers