Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b551 zirconium alloy in China. If you're going to wholesale high quality astm b551 zirconium alloy made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Zirconium Products Application
ASTM B551 Zirconium Alloy video
Chemical processing, aerospace, industrial, marine, smelting, chemical plants, plate heat exchangers and condensers, chemical and medical equipment.
Zirconium Material Specification
| Grade | Zr700 (R60700) | Zr702 (R60702) | Zr704 (R60704) | Zr705 (R60705) | Zr706 (R60706) |
| Component % | |||||
| Zr+Hf(min) |
99.2 |
99.2 |
97.5 |
95.5 |
95.5 |
| Hf(max) |
4.5 |
4.5 |
4.5 |
4.5 |
4.5 |
| Fe+Cr |
0.20(max) |
0.20(max) |
0.2-0.4 |
0.20(max) |
0.20(max) |
| Sn |
- |
- |
- |
1.0-2.0 |
- |


Like ASTM B551, ASME SB-551 is a standard specification for zirconium and zirconium alloy strip, sheet, and plate. It covers five grades: R60700 (low oxygen zirconium), Gr. R60702 (unalloyed zirconium), Gr. R60704 (Zr-Sn alloy), Gr. R60705 (Zr-Nb alloy), Gr. R60706 (zirconium niobium alloy) . Zirconium Ribbon: A flat product available in rolls less than 6 inches [150 mm] wide and 0.005 inches [0.13 mm] to 0.188 inches [4.8 mm] thick. Zirconium plate: A flat product with a width of 6 inches [150 mm] or more and a thickness of 0.005 inches [0.13 mm] to 0.188 inches [4.8 mm]. Zirconium Plate: A flat product over 0.125 inches [3.2 mm] thick.
Zr or Zr alloy strips, sheets and plates should be made from ingots produced by vacuum or plasma arc melting, vacuum electron beam melting and other methods. All processes should be carried out in furnaces used for reactive metals. The finished product is usually supplied in the recrystallized annealed state. Standard specifications also cover ordering information, chemical composition, mechanical properties, condition and surface treatment, permitted variations in dimensions and weight, workmanship and appearance, significance of numerical limits, number of tests and retests, sampling and test methods, inspection, rejection and Additional requirements for referees, certification, product marking, packaging and packaging markings, materials used for explosive cladding.
Customer Case
customer visit


FAQ
Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.
Q: What product information do I need to provide?
A: You need to provide the grade, width, thickness, coating and tonnage you need to purchase.
Q: What shipping ports are there?
A: Generally, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.
Q: About the product price of ASTM B551 Zirconium Alloy?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Hot Tags: astm b551 zirconium alloy, China astm b551 zirconium alloy suppliers
You Might Also Like
Send Inquiry