GB/T 3875 Tungsten Alloy Sheet
video

GB/T 3875 Tungsten Alloy Sheet

Tungsten is an invaluable element in the alloying process, where elements are blended to form new and improved metals known as alloys. Tungsten provides a unique contribution, as it imbues exceptional strength, corrosion resistance, and other useful properties to base metals. Besides being a great alloying element, tungsten can also be the base for its own alloys.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gb/t 3875 tungsten alloy sheet in China. If you're going to wholesale high quality gb/t 3875 tungsten alloy sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

GB/T 3875 Tungsten Alloy Sheet

The melting point and boiling point of Tungsten sheet are highest in all metals. There are three processing methods to produce tungsten sheet: hot rolling process, warm rolling process, cold rolling process. The processes of tungsten sheet production involve stamping, spinning, stretching, bending etc. The tungsten sheet has the properties of high density, internal stable structure and high temperature resistance.

Products Properties

 

Element Min Max Similar
W - - -
Total Others - 0.0180 -
Si - 0.0050 -
Others Each - 0.0020 -
O - 0.0050 -
Ni 4.8000 5.0000 -
N - 0.0030 -
Mg - 0.0030 -
H - 0.0010 -
Fe 2.0000 2.2000 -
Ca - 0.0050 -
C - 0.0080 -
Al - 0.0020 -
Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
451 (≥) 239 (≥) 44 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

GB/T 3875 Tungsten Alloy Sheet

GB/T 3875 Tungsten Alloy Sheet

Tungsten sheet Application:

Tungsten sheet is widely used in rotating anode of X-ray tube, heating element in high-temperature furnace, reflective shield, cover of the sapphire growth furnace, heat tape, heat insulation screen, vacuum coating equipment, high-temperature resisting boat.

 

Customer Case

 

GB/T 3875 Tungsten Alloy

FAQ

 

Q:What is an alloy?

A:An alloy is a mixture of metals or a metal made by combining two or more metallic elements. Alloys typically result in a product with greater strength or resistance to corrosion.

Q:What are the different alloys offered by TW Metals?

A:Titanium,Nickel,Aluminum,Stainless steel,Zirconium,Tantalum,Niobium,Tungstern.

Q:What kind of metal is an alloy?

A:Titanium,Nickel,Aluminum,Carbon

Q:What items are made from alloys?

A:Bar,Tube,Sheet,Plate,Pipe,Foil.

Q:What are metal alloys used for?

A:Metal alloys are used in a wide variety of applications. At TW Metals, we supply specialty metal products to the aerospace and commercial industries.

Hot Tags: gb/t 3875 tungsten alloy sheet, China gb/t 3875 tungsten alloy sheet suppliers, Tungsten Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry