ASTM B777 CLASS 1 Tungsten Pipe
video

ASTM B777 CLASS 1 Tungsten Pipe

Class 1 WHA (ET90) is the most commonly specified tungsten alloy. Typically, it is used for aerospace balance weights, medical shielding and other applications that require high density material.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b777 class 1 tungsten pipe in China. If you're going to wholesale high quality astm b777 class 1 tungsten pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

ASTM B777 CLASS 1 Tungsten Pipe

 

 

Class 1 material starts out as a blended metal powder (Pure W mixed with a binder of Ni and Iron). It is then pressed, sintered and in some cases machined into high quality tungsten heavy alloy (WHA) blocks, rods, and shaped parts. Although Class 1 has the lowest density, compared to Class 2, 3, & 4, it is still over twice the density of steels and most nickel-based super alloys.

Products Properties

 

 

Grade

ET90 ET90NM

ASTM B-777

Class 1

Class 1

AMS 7725E

Class 1 Type 2

Class 1 Type 1

MIL-T-21014D

Class 1

Class 1

W content, wt.%

90

90

Ni content, wt.%

7

8.9

Fe content, wt.%

3

1.1

Density, g/cm3

17

17

UTS, ksi

≥ 110

≥ 110

UTS, MPa

≥ 758

≥ 758

YS, ksi

≥ 75

≥ 75

YS, MPa

≥ 648

≥ 648

Elongation, % ≥ 5

≥ 5

Hardness, HRC

≤ 32

≤ 32

Mag. perm. > 1.05

≤ 1.05

ASTM B777 CLASS 1 Tungsten Pipe

ASTM B777 CLASS 1 Tungsten Pipe

Benefits of Class 1 WHA Material:

  • Environmental and density advantages over lead for radiation shielding
  • Unique capabilities for vibration dampening and balance weight applications
  • Ideal for applications requiring very high density
  • Excellent ability to absorb gamma rays and x-rays
  • Comparatively, it has improved machinability than pure tungsten
  • Excellent mechanical properties
Customer Case

 

ASTM B777 CLASS 1 Tungsten Alloy

 

FAQ

 

Q:What is an alloy?

A:An alloy is a mixture of metals or a metal made by combining two or more metallic elements. Alloys typically result in a product with greater strength or resistance to corrosion.

Q:What are the different alloys offered by TW Metals?

A:Titanium,Nickel,Aluminum,Stainless steel,Zirconium,Tantalum,Niobium,Tungstern.

Q:What kind of metal is an alloy?

A:Titanium,Nickel,Aluminum,Carbon

Q:What items are made from alloys?

A:Bar,Tube,Sheet,Plate,Pipe,Foil.

Q:What are metal alloys used for?

A:Metal alloys are used in a wide variety of applications. At TW Metals, we supply specialty metal products to the aerospace and commercial industries.

Q:What are metal alloys used for?

A:Metal alloys are used in a wide variety of applications. At TW Metals, we supply specialty metal products to the aerospace and commercial industries.

Hot Tags: astm b777 class 1 tungsten pipe, China astm b777 class 1 tungsten pipe suppliers, Tungsten Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry