ASTM B777 CLASS 4 Tungsten Alloy Pipe

Class 4 WHA material contains nominally, 97 weight percent (wt.%) Tungsten (W). Elmet’s Class 4 material is designated as ET97. A non magnetic (NM) alternative is not available in Class 4. ASTM B777 WHA, Class 4 provides a very high density material. It is easier to produce and machine relative to pure tungsten. Typically, Class 4 WHA is used for the most demanding X-Ray and radiation shielding applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b777 class 4 tungsten alloy pipe in China. If you're going to wholesale high quality astm b777 class 4 tungsten alloy pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

ASTM B777 CLASS 4 Tungsten Alloy Pipe

Class 4 material starts out as a blended metal powder (Pure W mixed with a binder of Ni and Iron). Then, it is pressed and sintered. The next step, in some cases, is to machine it into high-quality tungsten heavy alloy (WHA) blocks, rods, or other shaped parts. Notably, Class 4 has lower density compared to Pure Tungsten. However, it offers increased density over Class 1, 2 and 3. It also provides over twice the density of steels and most nickel-based super alloys. 

 

Products Properties

 

product-982-625

product-981-548

ASTM B777 CLASS 4 Tungsten Alloy Pipe

ASTM B777 CLASS 4 Tungsten Alloy Pipe

Class 4 WHA (ET95), is only used when the properties of Class 1, 2, and 3, for some reason, do not offer sufficient density or radiation or X-Ray shielding capability. While still machinable, Class 4 (ET97) is more difficult to machine than Class 1, 2 or 3.

Class 4 tungsten is a tungsten alloy. Cited properties are appropriate for the as-fabricated (no temper or treatment) condition. It has a fairly low heat capacity among alloys in the same category. In addition, it has a fairly high tensile strength and a fairly high density.
 

Customer Case

 

ASTM B777 CLASS 4 Tungsten Alloy

 

FAQ

 

Q: How long is your delivery time?
A: It is according to quantity. Generally it is 30 days.

Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Q:What are your payment terms?

A:30% T/T in advance and 70% balance before shipment or based on BL copy or LC at sight.

Q:What about product pricing information?

A:Prices vary due to changes in raw material prices on a regular basis.