TA1 Titanium Alloy Plate
video

TA1 Titanium Alloy Plate

TA1 is an industrial pure titanium alloy, also known as pure titanium TA1. It is composed of titanium with a purity higher than 99.5% and is one of the most common and basic pure titanium alloys.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ta1 titanium alloy plate in China. If you're going to wholesale high quality ta1 titanium alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

TA1 is an industrial pure titanium alloy, also known as pure titanium TA1. It is composed of titanium with a purity higher than 99.5% and is one of the most common and basic pure titanium alloys. TA1 has high strength, low density, excellent corrosion resistance and toughness. Its tensile strength is between 350-550MPa. It has good plasticity and is easy to process, shape and weld.

4 260

The excellent processing performance of TA1 allows it to be manufactured into structural parts of various shapes and sizes using a variety of processes, such as forging, rolling, drawing, etc. Moreover, it can also perform welding and cutting operations, providing more flexibility and possibilities for the manufacturing industry.

Specification TA1 Titanium Alloy Plate
Material TA1 Titanium Alloy
Thickness Range 0.5mm - 100mm
Width Range 1000mm - 2500mm
Length Range 2000mm - 6000mm or customized
Surface Finish Polished, Brushed, Matte, Sandblasted
Standard ASTM B265, ASME SB265
Applications Aerospace, Chemical Processing, Medical Implants, Marine Engineering
Features High strength-to-weight ratio, excellent corrosion resistance, biocompatibility
Composition Titanium (Bal.), Aluminum (2.5-3.5%), Vanadium (2-3%), Iron (0.3% max), Oxygen (0.2% max), Carbon (0.08% max), Nitrogen (0.05% max), Hydrogen (0.015% max)

219 06

Aerospace: TA1 is widely used in aircraft frames, skins, engine accessories and other components in the aerospace field. Its high strength, corrosion resistance and low density make it ideal as an aerospace material.


Ships and marine engineering: Because TA1 has excellent seawater corrosion resistance, it is often used to manufacture corrosion-resistant pipes, valves, pumps and other parts of ships. In addition, it can be used in desalination systems and other structural parts in marine projects.


Chemical industry: TA1 is widely used in the chemical industry to manufacture heat exchangers, pump bodies, distillation towers, coolers, mixers, tees and other corrosion-resistant equipment. It has excellent corrosion resistance under strong corrosive media and can provide reliable chemical equipment solutions.


Automobile industry: TA1 is often used in the automobile industry to manufacture pistons, connecting rods, leaf springs and other components of diesel engines. Its high strength and lightweight properties help improve engine performance and fuel economy.


Medical devices: Because TA1 has good biocompatibility with human tissue, it is widely used in the field of medical devices. For example, it can be used to make artificial joints, dental implants, surgical instruments, etc.


Other application fields: TA1 can also be used to manufacture mechanical equipment heat exchangers, golf clubs, etc. Its high strength, good corrosion resistance and lightweight properties make it an ideal structural material.

 