ASTM Titanium Alloy GR11 Round Bars
video

ASTM Titanium Alloy GR11 Round Bars

The composition element of Gr11 titanium rod is Ti-2Al-1.5Mn, which belongs to near-α titanium alloy, that is, an alloy with a β-stabilizing element content less than C1.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm titanium alloy gr11 round bars in China. If you're going to wholesale high quality astm titanium alloy gr11 round bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Titanium Products Application

ASTM Titanium alloy GR11 Round Bars video

Grade 11 titanium rods are widely used in extreme corrosive conditions in the following industries.

oil and gas industry
petrochemical plant
chemical plant
industrial machinery
Power Industry
Paper and pulp industry
food processing industry
refinery

Titanium Material Specification

 

Grade C N O H Ti Fe Al Pd
Titanium Gr 11 .08 max .03 max .25 max .015 max Bal 0.30 max - .12 - .25

ASTM Titanium alloy GR11 Round Bars

ASTM Titanium alloy GR11 Round BarsASTM Titanium alloy GR11 Round Bars

The composition element of Gr11 titanium rod is Ti-2Al-1.5Mn, which belongs to near-α titanium alloy, that is, an alloy with a β-stabilizing element content less than C1. The normal operating temperature range is 350 degrees, and the tensile strength is greater than or equal to 590MP.

Gr11 titanium rod is a type of titanium alloy. It has slightly higher performance and better process plasticity than pure titanium. It has both good welding performance and thermal stability. It cannot be strengthened by solid solution and aging. Can be used at high temperatures of 350 degrees. Long-term work, suitable for various plates, stampings, and welded parts, and suitable for manufacturing aviation sheet metal parts with complex shapes.

Customer Case

customer visit

ASTM Titanium alloy GR11 Round Bars

ASTM Titanium alloy GR11 Round Bars

FAQ

 

 

 

 

Q: How do you make our business establish a long-term and good relationship?
A: We maintain good quality and competitive prices to ensure that our customers benefit; we respect every customer just like our friends and sincerely do business and make friends with them. No matter where they come from.

Q: What is your delivery time?
A: Our delivery time is about one week, based on the number of customers.

Q: How long is your delivery time?
A: This is based on quantity. Generally it is 30 days.

Q: About the product price of ASTM Titanium alloy GR11 Round Bars?
A: Due to cyclical changes in raw material prices, prices vary in different periods.