Titanium Grade 2 CP 3 | UNS #R50400 is often referred to as the workhorse of commercially pure titanium grades and is therefore unalloyed.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of asme b348 round cp2 cp4 gr1 gr2 in China. If you're going to wholesale high quality asme b348 round cp2 cp4 gr1 gr2 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Titanium Products Application

ASME B348 Round CP2 CP4 GR1 GR2 video

Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubes, pickling baskets

Titanium Material Specification

 

MECHANICAL PROPERTIES
PROPERTY MINIMUM MAXIMUM
Yield Strength Range (Rp0.2 Offset) (ksi) 25 –
Tensile Strength Range (Rm) (ksi) 35 –
Elongation (AL=5 x Ø) 24.0% 29.0%
Brinell Hardness (H) – 120
Modulus of Elasticity (ksi) (E): 15200
Machineability General Index: 40%
 

ASME B348 Round CP2 CP4 GR1 GR2

ASME B348 Round CP2 CP4 GR1 GR2ASME B348 Round CP2 CP4 GR1 GR2

Titanium Grade 2 CP 3 | UNS #R50400 is often referred to as the workhorse of commercially pure titanium grades and is therefore unalloyed. Due to its varying availability and wider availability, this metal has been used in many markets and applications. Grade 2 titanium shares many similar qualities with grade 1 titanium, including corrosion resistance. However, level 2 is stronger.

Due to its high iron and oxygen content, Grade 2 titanium has high strength, good formability and weldability, and ductility. These properties make Grade 2 titanium rod and plate the first choice for a variety of applications.

Unalloyed commercially pure titanium or CP titanium. Grade 2 has higher iron and oxygen content than other CP grades, providing excellent formability and moderate strength with excellent corrosion resistance. CP grade 2 titanium is widely used in heat exchangers. CP2 is one of the most common titanium grades and its properties make it a good candidate for chemical, marine, aerospace and medical applications.

Customer Case

customer visit

ASME B348 Round CP2 CP4 GR1 GR2

ASME B348 Round CP2 CP4 GR1 GR2

FAQ

 

 

 

 

Q: How do you make our business establish a long-term and good relationship?
A: We maintain good quality and competitive prices to ensure that our customers benefit; we respect every customer just like our friends and sincerely do business and make friends with them. No matter where they come from.

Q: What is your delivery time?
A: Our delivery time is about one week, based on the number of customers.

Q: How long is your delivery time?
A: This is based on quantity. Generally it is 30 days.

Q: About the product price of ASME B348 Round CP2 CP4 GR1 GR2?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Hot Tags: asme b348 round cp2 cp4 gr1 gr2, China asme b348 round cp2 cp4 gr1 gr2 suppliers, Grade 2 Titanium Sheet Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry