Nickel 1.4462 1.4833 Pipe Stainless
video

Nickel 1.4462 1.4833 Pipe Stainless

1.4462 Duplex Plate is one of the most commonly used stainless steel alloys today. It has the moderate mechanical properties of a stainless steel alloy, making it useful in many applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 1.4462 1.4833 pipe stainless in China. If you're going to wholesale high quality nickel 1.4462 1.4833 pipe stainless made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 1.4462 1.4833 Pipe Stainless

Pressure vessels, high-pressure storage tanks, high-pressure pipelines, heat exchangers (chemical processing industry).

·Oil and gas pipelines, heat exchanger fittings.

Wastewater treatment system.

Classifiers, bleaching equipment, storage and handling systems for the pulp and paper industry.

Rotating shafts, press rollers, blades, impellers, etc. in high-strength and corrosion-resistant environments.

Ship or truck cargo box

food processing equipment

Nickel Material Specification

 

Chemical Composition

Grade C Mn P S Si Cr Mo Ni
Duplex 1.4462 0.03 max 2.0
max
0.035
max
0.015
max
1.0
max
21.0-
23.0
2.5-
3.5
4.5-6.5

Nickel 1.4462 1.4833 pipe stainless

Nickel 1.4462 1.4833 pipe stainlessNickel 1.4462 1.4833 pipe stainless

1.4462 Duplex Plate is one of the most commonly used stainless steel alloys today. It has the moderate mechanical properties of a stainless steel alloy, making it useful in many applications.
1.4833 heat-resistant steel is a high-temperature alloy steel with excellent heat resistance and mechanical properties. It is mainly composed of alloying elements such as chromium, nickel and molybdenum, giving it excellent corrosion and oxidation resistance. In addition, it has high strength and hardness, allowing it to maintain a stable structure in high-temperature environments. This kind of steel is widely used in petroleum, chemical, electric power and other industries, especially in working conditions under high temperature and high pressure environments. It is widely used in the manufacture of pipes, furnaces, heat exchangers, catalysts and petrochemical equipment. The production process of 1.4833 heat-resistant steel is also very mature. Electric arc furnace smelting and vacuum smelting technology are generally used to ensure the purity and uniformity of the steel. Then it undergoes hot rolling, forging, annealing and other processing processes to obtain the ideal structure and properties.