Nickel 200 Flanges contain nickel, iron, carbon, manganese, silicon, copper, magnesium, titanium, and sulfur elements. Nickel 200 flanges is a highly pure nickel alloy. Our main thought is to provide superior, high-quality, wondering products in different sizes, dimensions, and specifications per the customer's demand.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel 200 alloy pipe fittings flanges in China. If you're going to wholesale high quality nickel 200 alloy pipe fittings flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel 200 Flanges contain nickel, iron, carbon, manganese, silicon, copper, magnesium, titanium, and sulfur elements. Nickel 200 flanges is a highly pure nickel alloy. Our main thought is to provide superior, high-quality, wondering products in different sizes, dimensions, and specifications per the customer's demand.

1023 28

Nickel 201 Flanges is the central part of the connection of the pipes. These flanges are supplied to the customers from particular sections of industries like paper mills, sugar mills, fertilizer industry, breweries, petrochemical plants, fabrication units, and more. For the production of flanges, we use pure nickel with a low carbon quantity that makes the flanges work even at multiplied temperatures without any changes. Also, nickel 201 Flanges are made using top quality raw material and new equipment in production. As a result, Flanges include capabilities like a Long life period, High tensile, high durability, weldability, high flexibility, corrosion resistance, toughness, and strength in harsh environmental conditions.

Standard Werkstoff Nr. UNS JIS BS GOST AFNOR EN
Nickel 201 2.4068 N02201 NW 2201 NA 12 НП-2 – LC-Ni 99
Grade C Mn Si S Cu Fe Ni
Nickel 201 0.02 max 0.35 max 0.35 max 0.01 max 0.25 max 0.40 max 99.0 min

1023 55

Nickel 201 flanges offer excellent corrosion resistance in reducing and neutral media as well as in oxidizing atmospheres. Which provided the oxidizing media allows to the formation of a passive oxide film. These oxide alloys have excellent resistance to corrosion in an acidic environment. Nickel 201 is frequently used in environments containing alkalies, and it has changed its use in sulfuric, hydrochloric, anhydrous hydrofluoric, and non-aerated organic acids. This alloy is resistant to stress corrosion cracking in chloride salts, and it is ready to attack non-oxidizing halides. The concentration and temperature can be affected this alloy's resistance in certain environments. The all nickel alloy flanges of hot and cold working practices can be used to shape Nickel 201.