Uns N06600 Nickel Based Alloy tubing
video

Uns N06600 Nickel Based Alloy tubing

Available Formats
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
The alloy can be strengthened by cold working, and it can also be connected by resistance welding, solvent welding or brazing. It is suitable for making anti-oxidation parts that bear low load below 1100 ºC.

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06600 nickel based alloy tubing in China. If you're going to wholesale high quality uns n06600 nickel based alloy tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Uns N06600 Nickel Based Alloy tubing introduce

Uns N06600 Nickel Based Alloy tubing

Uns N06600 Nickel Based Alloy tubingUns N06600 Nickel Based Alloy tubing

Inconel600 is an early-developed nickel-chromium-iron-based solid solution strengthened alloy. It has good high temperature corrosion and oxidation resistance, excellent hot and cold processing and welding process performance, and has satisfactory heat resistance and high temperature below 700 ºC. Plasticity.

The alloy can be strengthened by cold working, and it can also be connected by resistance welding, solvent welding or brazing. It is suitable for making anti-oxidation parts that bear low load below 1100 ºC.

Inconel 600 Pipes & Tubes Equivalent Grades

Grade UNS DIN JIS BS GOST AFNOR EN
Alloy 600 N06600 2.4816 NCF 600 NA 13 МНЖМц 28-2,5-1,5 NC15FE11M NiCr15Fe

Inconel Alloy 600 Pipes & Tubes Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Alloy 600 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

GNEE Group Factory Environment

Uns N06600 Nickel Based Alloy tubing

Uns N06600 Nickel Based Alloy tubing

GNEE Group Product Packaging

Uns N06600 Alloy tubing

Uns N06600 Alloy tubing

FAQ

Q1:Can you assist me in importing steel products for the first time?
Yes, we have shipping agent who will arrange the shipment with you.
Q2. What is your delivery time?
Within 7 working days after receiving your balance payment.

Hot Tags: Uns N06600 Nickel Based Alloy tubing, China Uns N06600 Nickel Based Alloy tubing suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Monel 400 Alloy Steel Sheet, Hastelloy C 22 Alloy Steel Flange, 2 4668 Nickel Alloy Steel Coil, Hastelloy C276 ROUND BAR, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry