Nickel Based Alloy coil Inconel 625
video

Nickel Based Alloy coil Inconel 625

Available Formats
GNEE Group offers Nickel Alloy Inconel 625 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel based alloy coil inconel 625 in China. If you're going to wholesale high quality nickel based alloy coil inconel 625 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Nickel Based Alloy coil Inconel 625 introduce

Nickel Based Alloy coil Inconel 625

Nickel Based Alloy coil Inconel 625Nickel Based Alloy coil Inconel 625

GNEE STEEL is one of the renowned manufacturers, suppliers and exporters of these Inconel 625 Coils to accomplish various applications and operations. We manufacture these coils in large quantities and provide them as per the requirements and demands of our clients. These coils are in demand across various industries. These Inconel 625 contain a variety of metals like Molybdenum, Niobium, Chromium and Nickel alloys which provide excellent oxidation resistance and tensile strength. Inconel Coils have additional excellent fatigue capabilities and also exhibit stress corrosion cracking resistance to chloride ions. We offer Inconel 625 Coils in various sizes, shapes, dimensions and thicknesses. We also offer these coils in customized and non-customized forms.

Inconel N06625 Coils manufactured by us at GNEE STEEL are highly demanded in the market and we offer these Inconel 625 Coils at reasonable prices. We offer multiple benefits and features to our clients like it has excellent oxidation resistance and also has high rupture, creep and tensile strength, has excellent weldability and brazing, has optimum fatigue and thermal fatigue strength and also resists stress corrosion cracking from chloride ions, etc.

By following all national and international quality standards and defined manufacturing processes, we are manufacturing the right products. We are committed to satisfying the needs of our clients by offering quality Inconel 625 Coils to our valued customers. We use advanced technology and modern machinery to manufacture the products with the utmost precision and dimensionally accurate.

GNEE STEEL also takes care of the delivery of the products to the client's location. We pack these coils with suitable packing material and choose the fastest mode of transportation, ensuring timely delivery of the orders. We also keep coils in stock to meet the urgent needs of our valued customers.

Inconel 625 Coils Specification

Specifications : ASTM B443 / ASME SB443

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Thickness : 0.3 mm to 120 mm

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish : Hot rolled (HR), Cold rolled coils (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form : Plain Coils, Shim Coils, Strip, Flats, Blank (Circle), Ring (Flange)

Inconel 625 Coils Equivalent Grades

Grade WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 625 2.4856 N06625 NCF 625 NA 21 ХН75МБТЮ NC22DNB4M NiCr22Mo9Nb

Inconel 625 Coils Chemical Composition

Grade C Mn Si Cu S Cr Fe Ni N
Inconel Alloy 625 0.10 max 0.50 max 0.50 max - 0.15 min 20.0–23.0 5.0 max 58.0 min -

Inconel 625 Coils Mechanical Properties

Density Melting Point Tensile Strength Yield Strength 0.2% Proof Elongation (% in 50mm) (thick.>0.76mm)
8.4 g/cm3 1.350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

GNEE Group Factory Environment

Nickel Based Alloy coil Inconel 625

Nickel Based Alloy coil Inconel 625

GNEE Group Product packing

Nickel Based Alloy coil Inconel 625

product-800-390

GNEE Group customer visit

20231027152515

FAQ

1. how can we guarantee quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;
2.what can you buy from us?
Seamless pipe,stainless steel,carbon steel,Square tube,Profile
3. why should you buy from us not from other suppliers?
GNEE Steel Co., Ltd. is an enterprise specializing in the production of high-quality steel pipes, mainly producing stainless steel, seamless pipes, carbon steel, galvanized, profiles, etc. it is a professional one-stop steel product supplier.

 

Hot Tags: Nickel Based Alloy coil Inconel 625, China Nickel Based Alloy coil Inconel 625 suppliers, Uns N06600 Alloy tubing, Hastelloy C 22 Alloy Steel Flange, Ni36CrTiAl Plate, 2 4668 Nickel Alloy Steel Coil, Monel 400 Alloy Steel Sheet, Nickel Alloy Coil B2

Send Inquiry

whatsapp

Phone

E-mail

Inquiry