Monel 400 Nickel Based metal Alloy Plate
Length: upto 12000 mm
Thickness: 1 to 100 mm
Width: 1000 to 2500 mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 400 nickel based metal alloy plate in China. If you're going to wholesale high quality monel 400 nickel based metal alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel 400 metal Alloy Plate introduce
Monel 400 Nickel metal Alloy Plate


Monel 400 Sheets are a versatile alloy with excellent mechanical properties. They are commonly used in chemical processing and hydrocarbon handling equipment. They are also suitable for shafts, machinery and marine engineering. Monel 400 Sheets have a variety of corrosion resistance properties and are suitable for reducing environments.
Monel 400 Sheets are available in a variety of thicknesses. They are available in a variety of sizes and can be customized. We can provide Monel 400 Sheets and Monel 400 Sheets to your exact specifications. The high strength, corrosion resistance and ductility of this alloy make it ideal for many applications. Its ductility and low weight make it ideal for pressure sensitive components.
Monel 400 Sheets and Plates Specification
Specifications :ASTM B127 / ASME SB127, AMS 4544
Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc
Length : 2000mm, 2440mm, 3000mm, 5800mm, 4000mm, etc
Thickness : 0.3 mm to 120 mm
Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Form : Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Monel Alloy 400 Sheets & Plates Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel 400 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
GNEE Group Factory Environment
Monel 400 Nickel Based Alloy Plate

GNEE Company Environment
Monel 400 Nickel Alloy Plate

FAQ
1. how can we guarantee quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;
2.what can you buy from us?
Seamless pipe,stainless steel,carbon steel,Square tube,Profile
3. why should you buy from us not from other suppliers?
GNEE Steel Co., Ltd. is an enterprise specializing in the production of high-quality steel pipes, mainly producing stainless steel, seamless pipes, carbon steel, galvanized, profiles, etc. it is a professional one-stop steel product supplier.
Hot Tags: Monel 400 Nickel Based metal Alloy Plate, China Monel 400 Nickel Based metal Alloy Plate suppliers, Cold Rolled Inconel 625 Alloy Seamless Pipe, Hastelloy C276 ROUND BAR, Ni36CrTiAl Plate, Uns N06600 Alloy tubing, Hastelloy C 22 Alloy Steel Flange, Alloy Steel 600 plate