GH3030 Plate
Finish:2B, 2D, BA NO(8)
Form:Sheets, Plates
Hardness:Soft, Hard, Half Hard
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
- Tel: +8615824687445
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3030 plate in China. If you're going to wholesale high quality gh3030 plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH3030 Plate description
Gnee Steel is a leading manufacturer, supplier, and exporter of GH3030 alloy plates and sheets. We use high-quality raw materials and meticulously manufacture and process our products to meet domestic and international standards. The nickel-chromium alloy in GH3030 plates offers excellent high-temperature oxidation resistance. Furthermore, they exhibit superior resistance to chloride ion stress corrosion cracking, high-purity water corrosion, and acidic environment erosion.

GNEE High Temperature Alloy GH3030 Sheet
GH3030 is a nickel-chromium-based solid solution strengthened superalloy (equivalent to Nimonic 75). It is specifically designed for applications requiring extremely high-temperature oxidation resistance and excellent formability. GH3030 sheet metal can operate at temperatures up to 800°C under structural loads and offers oxidation resistance up to 1000°C, making it ideal for combustion chamber linings and heat-treated fixtures.
Gnee Steel supplies high-quality GH3030 sheet metal, perfectly balancing ductility, weldability, and thermal stability to ensure your components can withstand the most demanding thermal cycling environments.



Gnee Steel offers premium GH3030 alloy steel sheets in a variety of sizes and thicknesses, and provides custom cutting, finishing, and worldwide delivery services to meet your specific project needs.
Request a quote for a custom shape
GH3030/Nimonic 75 Plate Specification
| Specifications of GH3030 PLATES / SHEETS: |
| Grade | GH3030 |
| Thickness | 0.1mm To 100 mm |
| Size | 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
| Form | Sheets, Plates, Coils, Slatting Coils, Perforated Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange) |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Alloy GH3030 Plate Specification
| EQUIVALENT GRADES OF GH3030 PLATES / SHEETS/COIL: |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| GH3030 | - | - | - | NA 11 | МНЖМц 28-2,5-1,5 | NC15FE11M | NiCr15Fe |
| CHEMICAL COMPOSITION OF GH3030 PLATES / SHEETS/COIL: |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| GH3030 | 0.12 max | 0.70max | 0.80 max | 0.02max | - | 1.5 | balance | 19.00 – 22.00 |
GH3030 Sheet Physical Properties
| Property | Value |
|---|---|
| Density | 8.4 g/cm³ |
| Melting Point | 1374 - 1420 °C |
GH3030 Sheet Mechanical Properties
| Status | Tensile Strength (Rm N/mm²) | Yield Strength (Rp 0.2 N/mm²) | Elongation (%) | Brinell Hardness (HB) |
|---|---|---|---|---|
| Solution Treatment | 785 | – | 35 | – |
Click to download the GH3030 alloy PDF file now
GH3030 Plate Available Sizes and Supply Range

GH3030 Sheet Sizes
We stock and manufacture GH3030 in various thicknesses to support both precision instrumentation and heavy industrial machinery.
| Item | Thickness (mm) | Width (mm) | Length (mm) | Finish |
| Cold Rolled Sheet | 0.5mm – 4.0mm | 600 – 1000 | 2000 – 3000 | Bright, Pickled |
| Hot Rolled Plate | 4.0mm – 50.0mm | Up to 2000 | Up to 6000 | Pickled, Sandblasted |
Nimonic 75 Plate Manufacturing Process

Alloy GH3030 Plate Manufacturing Process
GH3030 Sheet Manufacturing Process and Quality Control
Our GH3030 sheet manufacturing process ensures fine grains and uniform thickness:
VIM + ESR Melting: Vacuum induction melting followed by electroslag remelting to obtain ultra-clean metal.
Cross-rolling technology: Ensures isotropic mechanical properties (uniform longitudinal and transverse strength).
Strict solution annealing: Controlled heating at 1130°C, followed by rapid quenching to lock in the solid solution state.
Flatness control: Precision leveling ensures the sheet meets the requirements of automated laser cutting machines.
The delivery time for Alloy XH78T Plate varies depending on the location
| Cost Changes 5 % extra | |
|---|---|
| Export to | Delivery Time |
| UAE | 5 days |
| Qatar | 7 |
| France | 30 |
| Kuwait | 10 |
| USA | 40-60 |
| Saudi Arabia | 7 |
| Oman | 5 |
| Italy | 30 |
| Uk | 30 |
Products and services offered by Gnee Steel
GH3030 Sheet Main Applications
GH3030 sheet is the preferred material in the following fields:
Aero-engines: Combustion chamber shells, flame tubes, and mounting rings.
Industrial furnaces: Muffle furnace plates, furnace linings, conveyor belts, and radiant tube shells.
Chemical equipment: High-temperature reactor linings and heat exchanger plates.
Automotive: Turbocharger housings and exhaust heat shields.






Packaging method for Alloy GH3030 Plate
Standard export sea freight packaging:
Waterproof paper wrapping + PVC film + strapping + wooden pallet or wooden crate;
Customized packaging according to your requirements (logos or other content printed on the packaging are acceptable);
Other special packaging will be designed according to customer requirements;
Air or sea freight;
Port of shipment: Shanghai, Tianjin, or as per your requirements.
About Gnee Steel

Choose Gnee Steel, choose reliability. We combine the technical precision of a manufacturer with the agility of a global distributor.
Global Fast Shipping: Air freight (3-5 days) or sea freight (20-30 days).
Technical Support: Contact our metallurgical engineers directly for material selection.
Price Guarantee: All high-temperature alloys are offered at highly competitive factory-direct prices.

Please contact us to get a quick quote for the Nimonic 75 Plate you need
We supply these Alloy GH3030 Plate according to DIN, ISO, JIS, or ANSI/ASME standards.
FAQ
Q1: What is the difference between GH3030 and GH3128?
A: GH3030 is a simpler Ni-Cr alloy primarily for oxidation resistance and formability. GH3128 is more complex (with W and Mo), offering higher creep strength at temperatures above 900°C. GH3030 is generally more cost-effective for components under 800°C.
Q2: Can GH3030 plates be used in sulfur-rich environments?
A: Like most high-nickel alloys, GH3030 is susceptible to sulfidation in reducing atmospheres. It performs best in oxidizing or neutral atmospheres. For sulfur-rich environments, please contact our experts for specialized coating or alloy recommendations.
Q3: How do you handle surface protection during shipping?
A: We use PVC film coating for cold-rolled sheets to prevent scratches, and all plates are packed in seaworthy wooden crates with moisture-absorbent silica gel.
Q4: Do you provide a Mill Test Certificate (MTC)?
A: Yes, every shipment includes a full MTC showing chemical analysis, mechanical tests, and grain size inspection according to EN 10204 3.1.
Hot Tags: gh3030 plate, China gh3030 plate suppliers, component alloy, heat resistant alloy, machinery alloy, quality alloy, strong alloy, wear resistant alloy
Previous
GH3030 BarNext
GH3030 PipeYou Might Also Like
Send Inquiry