Name: ASTM B163 UNS N02201 Alloy Seamless Pipe
Approximate grades:NO2201,Nickel201,Ni201,N5
Shape:Round
Technique:Cold Rolled
Surface Treatment:Pickling
Tolerance:-+10%
Processing Service:Bending, Welding, Decoiling, Punching, Cutting
Pipe Form Type:Seamless Steel Pipe
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b163 uns n02201 alloy seamless pipe in China. If you're going to wholesale high quality astm b163 uns n02201 alloy seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B163 UNS N02201 alloy seamless pipe‌ is a high-quality seamless pipe used for condensers and heat exchangers. The main materials are nickel and nickel alloys, which have high purity, high thermal conductivity and corrosion resistance.
‌
‌Nickel 201 Hollow Pipe Application‌
It is widely used in chemical equipment, marine engineering, high-temperature furnaces, jet engines, steam generators and other fields that require long-term contact with corrosive substances or high-temperature environments.

 Nickel Alloys 201 Specification
Product Name Nickel Alloy 201 Pipe
Outside diameter Round tube

4mm-200mm

Square tube

10*10mm-100*100mm

Rectangular tube

10*20mm-50*100mm

Wall thickness

0.6mm-6.0mm

length 1-6 meters, length can be customized
standard

ASTM / AISI / JIS / GB / DIN / EN

surface Black, bright polishing, rough turning, matte surface treatment, NO.4, BA, etc.
Certificate

ISO / SGS / BV

Production Technology Hot Rolled / Cold Rolled

 

‌Nickel 201 seamless straight tubing Physical properties

 

Units

Temperature in°C

Density

8.9 g/cm³

Room

Specific Heat

0.105 Kcal/kg.C

Room

Melting Range

1435-1445 °C

-

Modulus of Elasticity

207 KN/mm²

Room

Electrical Resistivity

8.5 µΩ.cm

20°

Coefficient of Expansion

13.3 µm/m °C

20 - 100°

Thermal Conductivity

67.1 W/m -°K

20°

 

 Alloys 201 Products Display

201 Nickel Alloy Round Pipe

201 Nickel Alloy Round Pipe

Why choosing GNEE

GNEE specializes in the production of high temperature (nickel-based) alloys, austenitic, duplex steel, super austenitic stainless steel and other products.
GNEE has 38 online fully automatic welding units. The production range of online automatic welding round pipes is: 8mm-1067mm; wall thickness range: 1mm-14mm; length: 1.0-12 meters; it can be customized according to customer requirements.

please contact us for a quote! ss@gneesteel.com

PRODUCTS TESTING

PRODUCTS TESTING

Nickel DIN 2.4068 Seamless Pipes Exporter

Nickel  201 Alloy Manufacturer

 Alloy 201 Seamless Pipe Manufacturer

 Superalloys 201 Pipe Supplier, Stockist

FAQ

Q:What about product pricing information?
Prices vary due to changes in raw material prices on a regular basis.

Q:Is it possible to send samples?
Of course, we offer free samples and express shipping to customers all over the world.

Q:Do you offer a service for customized products?
Yes, we can produce according to your specifications and drawings.

Hot Tags: astm b163 uns n02201 alloy seamless pipe, China astm b163 uns n02201 alloy seamless pipe suppliers, Monel 400 Alloy Steel Sheet, Cold Rolled Inconel 625 Alloy Seamless Pipe, 2 4668 Nickel Alloy Steel Coil, Alloy Steel 600 plate, Hastelloy C276 ROUND BAR, Uns N06600 Alloy tubing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry