As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 59 / 2.4605 in China. If you're going to wholesale high quality alloy 59 / 2.4605 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
The nickel-chromium-molybdenum Alloy 2.4605 (alloy 59) is often used for chemical industry, pulp and paper industry as well as flue gas desulfurization plants. E are able to deliver tubes, tube accessories, flanges, rods and bars as well as sheets and plates in 2.4605 (Alloy 59). Alloy 59 is stated in BAM-List (Hazardous Materials Transportation).
Material
Application
Composition
Characteristics
Delivery program
Outlet
Material Data Sheet
| Material Designation | 2.4605 |
| Alloy | Alloy 59 |
| EN Material Symbol | NiCr23Mo16Al |
| UNS | N 06059 |
| Trademark | Nicrofer® 5923hMo |
| Norm DIN | EN 17744 |
| VdTÜV Technical Data Sheet | 505 |
Main fields of application of alloy 59
Alloy 59 is used for: environmental technology, chemical industry (chemical processes with oxidating and reducing acids, resistance against damp chloric gas) and solid waste incinerators. Predominantly 2.4605 is used for chemical industry, pulp and paper industry and and flue gas desulfurization plants.
Chemical composition of alloy 59
| C | Si | Mn | P | S | Cr |
| ≤ % | ≤ % | ≤ % | ≤ % | ≤ % | % |
| 0.01 | 0,1 | 0,50 | 0,025 | 0,015 | 22,0-24,0 |
| Mo | Ni | Al | Co | Cu | Fe |
| % | % | % | ≤ % | ≤ % | ≤ % |
| 15,0-16,0 | Rest | 0,10-0,40 | 0,30 | 0,50 | 1,50 |
Characteristics of alloy 59
| Temperature Range | Material for wet corrosion |
| Density | 8,6 g/cm³ |
| ISO-V notch impact toughness | ≥ 225 J/cm² at room temperature |
| ≥ 200 J/cm² bei -196°C | |
| Low sensitivity for intercrystalline corrosion |
Delivery program
| Rods and Bars: | 8 – 85/115sq mm |
| Sheets and Plates: | 2 – 40 mm |
| Coils: | 2 mm |
| Elbows: | OD 48,3 – 88,9 mm |
| Tubes: | OD 10,2 – 273 mm |
With short delivery time:
plates or sheets, tubes, flanges, forged or die-cut rings and round blanks, elbows, T-fittings, reductions, screws, nuts or washers according to your request. According to your individual wishes, we are able to cut our material with our plasma- or water jet cutter. Our material is stocked in superformats of 2000x6000mm. Cut to size on request.




FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: alloy 59 / 2.4605, China alloy 59 / 2.4605 suppliers, 2 4668 Nickel Alloy Steel Coil, Monel 400 Alloy Steel Sheet, Alloy Steel 600 plate, Cold Rolled Inconel 625 Alloy Seamless Pipe, Ni36CrTiAl Plate, Hastelloy C 22 Alloy Steel Flange
You Might Also Like
Send Inquiry