AL-6XN UNS N08367 Pipe Stainless Steel Seamless
video

AL-6XN UNS N08367 Pipe Stainless Steel Seamless

AL6XN is a super austenitic stainless steel with excellent resistance to chloride pitting, crevice corrosion and stress corrosion cracking. AL6XN is a 6-molybdenum alloy developed specifically for use in highly corrosive environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of al-6xn uns n08367 pipe stainless steel seamless in China. If you're going to wholesale high quality al-6xn uns n08367 pipe stainless steel seamless made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

AL-6XN UNS N08367 Pipe Stainless Steel Seamless

AL-6XN stainless steel plays an important role in many industries. In the field of marine engineering, it is widely used in the manufacture of seawater treatment equipment, pipeline systems and storage tanks. Due to its excellent corrosion resistance, it can effectively resist corrosion and erosion in seawater, thereby extending the service life of the equipment.

In the chemical and oil and gas industries, AL-6XN stainless steel is widely used to manufacture equipment such as reactors, heat exchangers, and storage tanks. These devices are often found in extremely corrosive environments and require materials with excellent corrosion resistance and mechanical strength. AL-6XN stainless steel is one of the materials that meets these requirements.

In addition, AL-6XN stainless steel is also widely used in the food processing and pharmaceutical industries. Due to its highly reliable corrosion resistance, it can be used to manufacture food processing equipment and pharmaceutical production equipment to ensure product quality and safety.

In short, AL-6XN stainless steel, as a high-performance corrosion-resistant alloy, plays an important role in many industries. Its excellent corrosion resistance, mechanical strength and processability make it the material of choice for a variety of applications. With the continuous advancement of science and technology, I believe that AL-6XN stainless steel will play a greater role in more fields and make more breakthroughs.

super alloy Material Specification

 

Ni Cr Mo C N Mn Si P S Cu Fe

23.5-25.5

20.00-22.00

6.00-7.00

0.03 Max

0.18-0.25

2.0 Max

1.00 Max

.040 Max

0.03 Max

0.75 Max

Remainder

Hot Tags: al-6xn uns n08367 pipe stainless steel seamless, China al-6xn uns n08367 pipe stainless steel seamless suppliers, component alloy, heat resistant alloy, Monel R405, turbine alloy, Monel N04400 N05500 Thick Wall Pipe, tough alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry