SUS317L Stainless Steel Round Bar ASTM 317L Uns S31703 Sts317L 1.4438 AISI 317L
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus317l stainless steel round bar astm 317l uns s31703 sts317l 1.4438 aisi 317l in China. If you're going to wholesale high quality sus317l stainless steel round bar astm 317l uns s31703 sts317l 1.4438 aisi 317l made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
it has good corrosion resistance, heat resistance, low temperature strength and mechanical properties, punching, bending, such as hot workability is good, no heat treatment hardening phenomenon.
Purpose: tableware, ambry, boiler, auto parts, medical appliances, building materials, food industry (using the temperature - 196 ° C to 700 ° C)
has good corrosion resistance, heat resistance, low temperature strength and mechanical properties, punching, bending, such as hot workability is good, no heat treatment hardening phenomenon.
Purpose: tableware, ambry, boiler, auto parts, medical appliances, building materials, food industry (using the temperature - 196 ° C to 700 ° C)
| Product Name | ASTM 317L 022Cr19Ni13Mo3 SUS317L S31703 stainless steel round bar |
| Type | Round Bar |
| Surface | Black,bright,rough turned,grinding,centreless Ground etc |
| Standard | GB,AISI,ASTM,DIN,EN,SUS,UNS etc |
| Diameter | 4-800mm |
| Technigue | Hot Rolled,Cold Rolled,Cold Drawn,Forged |
| Testing Methods | Flaw detection, Eddy current testing, Hydrostatic testing or Ultrasonic examination and also with chemical and physical property inspection |
| Grade | 200 series: 201,202,202Cu,204Cu, 300 series: 301,303/Cu,304/L/H,304Cu,305,309/S,310/S,316/L/H/Ti,321/H,347/H,330, 400 series: 409/L,410,416/F,420/F,430,431,440C,441,444,446, 600 series: 13-8ph,15-5ph,17-4ph,17-7ph(630,631),660A/B/C/D, Duplex: 2205(UNS S31803/S32205),2507(UNS S32750),UNS S32760,2304,LDX2101.LDX2404,LDX4404,904L Others: 153Ma,254SMo,253Ma,654SMo,F15,Invar36,1J22,N4,N6 etc |
| Third Party Inspection | SGS BV MTC |
| Trade Terms | FOB CIF CFR |
| Payment TermsFOB 30%T/T,70% before shipment CIF 30% pre-payment and the balance to be paid upon B/L (copy) or Irrevocable 100% L/C at sight |
|
GENERAL PROPERTIES
Alloy 317L is a molybdenum containing, low carbon austenitic stainless steel with increased additions of chromium, nickel, and molybdenum for better corrosion resistance and increased resistance to chemical attack for sulfurous, acetic, formic, citric, and tartaric acids. Due to its low carbon content, 317L also provides resistance to sensitization when welded and higher creep, stress to rupture, and tensile strength at elevated temperatures. It is non-magnetic in the annealed condition but may become slightly magnetic after welding.
APPLICATIONS
Alloy 317L is commonly used to handle sulfur, pulp liquor, acid dyestuffs, acetylating and nitrating mixtures, bleaching solutions, severe coal and oil, and many chemical compounds. Some other applications that use alloy 317L include:
Paper and pulp handling equipment
Chemical and petrochemical processing equipment
Condensers in fossil and nuclear fueled power generation stations
Food processing equipment
Textile equipment
STANDARDS – ALLOY 317L
ASTM/ASME: UNS N08020
EURONORM: FeMi35Cr20Cu4Mo2
DIN: 2.4660
CORROSION RESISTANCE
Demonstrates superior corrosion resistance in difficult environments including a wide range of chemicals, especially in acidic chloride environments
Excellent resistance in applications where contamination is desired to be kept to a minimum
Low carbon content allows 317L to be highly resistant to intergranular corrosion
Combats the tendency to pit when in contact with phosphorus acids, chlorides, bromides, and iodides
HEAT RESISTANCE
All chromium-nickel-molybdenum steels all have excellent resistance to oxidation
Demonstrates a low rate of scaling in ordinary atmospheres at temperatures up to 1600-1650°F (871-899°C).
Chemical Properties:
| % | Cr | Ni | C | Si | Mn | P | S | Mo | Fe |
|---|---|---|---|---|---|---|---|---|---|
| 317L | min: 18.0 max:20.0 |
min: 11.0 max: 15.0 |
0.035 max |
0.75 max |
2.0 max |
0.04 max |
0.03 max |
min: 3.0 max: 4.0 |
balance |
Mechanical Properties:
| Grade | Tensile Strength ksi (min.) |
Yield Strength 0.2% Offset ksi (min.) |
Elongation - % in 50 mm (min.) |
Hardness (Brinell) MAX |
Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 317L | 75 | 30 | 40 | 217 | 95 |
Physical Properties:
| Denstiy lbm/in^3 |
Coefficient of Thermal Expansion (min/in)-°F |
Electrical Resistivity mW-in | Thermal Conductivity BTU/hr-ft-°F | Specific Heat BTU/lbm -°F | ||
|---|---|---|---|---|---|---|
| at 68 °F | at 77 – 212°F | at 77 – 932°F | at 77 – 1832°F | at 68 – 1832°F | at 32 – 212°F | |
| 0.29 | 9.2 | 10.1 | 10.8 | 31.1 | 14.6 | |
FAQ
1. How can I get a quotation from you?
You can leave us a message, and we will reply to every message in time. Or we may talk online by Trademanager.
And you can also find our contact information on the contact page.
2.Can I get samples before order?
Yes, of course. Usually, our samples are free. we can produce your samples or technical drawings, all you need to pay is the shipping cost to you. We can build moulds and fixtures so we can customize our products based on your demand.
3. what is your delivery time?
It mainly depends on your location and demanded volume. The time of delivery is usually around 1 month(1*40FT as usual).
We can send it out in 2 days if it has stock.
4.What is your payment terms?
Our usual payment term is 30% deposit and the rest against B/L. L/C is also acceptable. And the shipping terms are EXW, FOB, CFR, CIF and DDU. Whichever you like.
5. How can you guarantee the quality of my goods?
We are a factory with 100% pre-delivery inspection which guarantee the quality.
6 How do you make our business long-term and good relationship?
1. We keep good quality and competitive price to ensure our customers benefit ;
2. We respect every customer and we sincerely do business with them, sustain our service level before and after every deal.
Hot Tags: sus317l stainless steel round bar astm 317l uns s31703 sts317l 1.4438 aisi 317l, China sus317l stainless steel round bar astm 317l uns s31703 sts317l 1.4438 aisi 317l suppliers, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar
You Might Also Like
Send Inquiry