SS 1.4529 Pealed Stainless Steel Round Bar EN 10088 3 Diameter 30 Mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 1.4529 pealed stainless steel round bar en 10088 3 diameter 30 mm in China. If you're going to wholesale high quality ss 1.4529 pealed stainless steel round bar en 10088 3 diameter 30 mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Machinery Accessories Dedicated 1.4529/N08367 Stainless Steel Round Bar
Chemical composition(mass fraction)(wt.%) of the 1.4529
| C | Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| ≤0.020 | 1.00 | 2.00 | 0.030 | 0.015 | 19.0-21.0 | 24.0-26.0 | 6.00-7.00 | N 0.15-0.25 Cu 0.50-1.50 |
Mechanical properties / Mechanische Eigenschaften / Caracteristiques mecaniques of grade 1.4529
MECHANICAL PROPERTIES
PHYSICAL PROPERTIES
HEAT TREATMENT
MORE
| Yield Rp0.2(MPa) |
Tensile Rm(MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 131 (≥) | 823 (≥) | 21 | 24 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 |
Stainless Steel - grade 1.4529
EN1.4529
AISI926
UNSN08926
DINX1NiCrMoCuN25-20-7
StructureSuper-Austenitic
Composition
C: max. 0,02%
Cr: 19,0-21,0%
Cu: 0,50-1,50%
Mn: max. 1,00%
Mo: 6,00-7,00%
Ni: 24,0-26,0%
P: max. 0,030%
S: max. 0,010%
Si: max. 0,50%
Balance: N 0,15-0,25%
Applications
Plant manufacturing
Petro chemical
Construction
Ship building
Machine engineering
Delivery form
Plate, cold rolled
Plate, hot rolled
Roundbar, rolled
Flatbar, cold rolled
welded pipe/ welded tube
Forgings
laser cuts
plasma cuts
waterjet cuts
saw cuts
Rings
Discs
Tailormade drawings
Bored roundbars
Product details


Packing & shipping


Hot Tags: ss 1.4529 pealed stainless steel round bar en 10088 3 diameter 30 mm, China ss 1.4529 pealed stainless steel round bar en 10088 3 diameter 30 mm suppliers, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes
You Might Also Like
Send Inquiry