Nickel EN Alloy Round Bar Gh5188 / Gh188 / Haynes Alloy No. 188/Haynes188/ Unsr30188
video

Nickel EN Alloy Round Bar Gh5188 / Gh188 / Haynes Alloy No. 188/Haynes188/ Unsr30188

GH5188 solution-strengthening cobalt-based superalloy, adding 14% tungsten solid solution strengthening, makes the alloy have excellent high-temperature thermal strength, adding high content of chromium and trace lanthanum, so that the alloy has good high-temperature oxidation resistance, and has Satisfactory forming, welding and other process properties, suitable for manufacturing aero-engine parts that require high strength below 980°C and anti-oxidation below 1100°C. It can also be used on aerospace engines and space shuttles. It can produce and supply various deformed products, such as sheet, medium plate, strip, bar, forging, wire and precision casting.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of nickel en alloy round bar gh5188 / gh188 / haynes alloy no. 188/haynes188/ unsr30188 in China. If you're going to wholesale high quality nickel en alloy round bar gh5188 / gh188 / haynes alloy no. 188/haynes188/ unsr30188 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Product Description

Nickel Alloy Gh5188 / Gh188 / Haynes Alloy No. 188/Ha188/ Unsr30188 / Kcn22W / High Temperature Alloy Forged Alloy Steel Round bar & Rods


GH5188 solution-strengthening cobalt-based superalloy, adding 14% tungsten solid solution strengthening, makes the alloy have excellent high-temperature thermal strength, adding high content of chromium and trace lanthanum, so that the alloy has good high-temperature oxidation resistance, and has Satisfactory forming, welding and other process properties, suitable for manufacturing aero-engine parts that require high strength below 980°C and anti-oxidation below 1100°C. It can also be used on aerospace engines and space shuttles. It can produce and supply various deformed products, such as sheet, medium plate, strip, bar, forging, wire and precision casting.

1.1 GH5188 (GH188) material grade GH5188 (GH188).

1.2 GH5188 (GH188) similar grades Haynes Alloy No.188 (HA188), UNSR30188 (USA), KCN22W (France).


UNS R30188

Chemical composition

% Co Ni Cr W Fe C Mn Si P S La B
min balance 20.0 20.0 13.0  
0.05
  0.20    
0.02
 

max
24.0 24.0 16.0 3.0 0.15 1.25 0.50
0.020

0.015

0.12

0.015


Physical properties

Density 8.98 g/cm3
Melting range 1315-1410ºC

 

 

FAQ

Question: Are you a trading company or manufacturer?
Answer: We're manufacturer.

Question2: Could you help to design the product?

Answer: Yes, we have excellent R&D team, OEM/ODM orders are all welcome.

 

Question: Could you supply samples?

Answer: Yes, wecould supply samples according to your requirement.


Question: could we visit your factory?
Answer: Sure, factory visit is warmly welcome.

Nickel EN Alloy Round Bar Gh5188 / Gh188 / Haynes Alloy No. 188/Haynes188/ Unsr30188 0Nickel EN Alloy Round Bar Gh5188 / Gh188 / Haynes Alloy No. 188/Haynes188/ Unsr30188 1Nickel EN Alloy Round Bar Gh5188 / Gh188 / Haynes Alloy No. 188/Haynes188/ Unsr30188 2

Hot Tags: nickel en alloy round bar gh5188 / gh188 / haynes alloy no. 188/haynes188/ unsr30188, China nickel en alloy round bar gh5188 / gh188 / haynes alloy no. 188/haynes188/ unsr30188 suppliers, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 420 Stainless H type Steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry