SAE1020 ASTM Cold Drawn Bright Round Bar Ss400 A36 S45c Sae1045 42CrMo
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sae1020 astm cold drawn bright round bar ss400 a36 s45c sae1045 42crmo in China. If you're going to wholesale high quality sae1020 astm cold drawn bright round bar ss400 a36 s45c sae1045 42crmo made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SAE1020 ASTM Cold Drawn Bright Round Bar Ss400 A36 S45c Sae1045 42CrMo
Description
| Steel Grade: | Ss400 A36 S45c Sae1045 42CrMo | Alloy Or Not: | Non-alloy |
|---|---|---|---|
| Technique: | Hot Rolled,Cold Drawn | Application: | Structural Steel Bar |
| Type: | Carbon Steel Bar | Standard: | ASTM,DIN,AISI,JIS |
| Shape: | Round | Length: | 1--12m |
| Surface: | Black Or Bright | Diameter: | 12mm-650mm |
| High Light: |
forged steel round bar,bright steel round bar |
||
Cold Drawn SAE1020 Round Bar ASTM A36 Cold Drawn Bright Round Bar
1045 quenched & tempered qt steel bar
1045 is a medium carbon steel for mechanical engineering and automotive components manufacturing. It can get high strength and high hardness after quenched and tempering. The similar material includes C43, C44, C45E, CK45, SAE1045, 080A42, S45C ETC.
Quenching and Tempering, abbreviated as Q&T is a king of processing that strengthen or harden steel bars by heating the materials and then cooling in water, oil or other liquid medium, that rapidly the change from austenite to perlite to get the proper properties for various usage. The quenched & tempered steel bar materials are usually with carbon from 0.30% - 0.60%, it is widely used as merchant bars in components of various machines.
1045 material quenched and tempered q&t steel bar we supply includes following advangtages:
Consistent mechanical properties
Deep mechanical properties (from surface to the center according to your requirement)
Even hardness on the whole bars/Tougher and Increased strength
No brittle, UT testing/Precision size tolerance/Good straightness
Good Roughness/Professional technical service/Competitive price/Fast delivery
Specification of 1045 material quenched and tempered q&t steel bar we supply:
1. 1045 steel equivalent material:
| GB | ASTM/SAE/AISI | DIN | SCM | AS /NZS1444 |
| 45# | Aisi 1045 / sae 1045 / astm 1045 | C45 CK45 | S45C | AS 1045 |
2. C45 steel chemical composition:
| Material | Chemical Composition % | ||||||
| C | Si | Mn | S | P | Cr | Mo | |
| 1045 | 0.42-0.48 | 0.15-0.35 | 0.60-0.90 | 0.035 max | 0.035 max | 0.035 max | 0.035 max |
3. 1045 QT steel mechanical properties:
| Mechanical Properties | ||||
| Yield Strength (MPa) | Tensile Strength (MPa) | Elongation | Reduction of area | Hardness |
| 830 min | min660 | 12% min | 45% min | 32HRC max |
4. 1045 steel applications:
high strength stud bolt, Threaded Rods, wind power bolt, prestressed anchor bolts, post stressed anchor bolt, Steel Tie Rod, tie bar, tension rod, Tension Bar etc. Shaft, axle shaft, crankshaft, shaft for sleeve, linear shaft, pump shaft, rotor shaft, sensor shaft, spline shaft, drive shaft, mandrel shaft, transmission shaft, screw rod etc. CNC machines, precision CNC machines etc. Ejector pins and Ejector rods
5. Production line:

6. Production Facilities:

7. Inspection:

8. Package:

9. RFQ:
Q1. Are you a manufactuer?
A1:Yes, we have our own factory and labatory to produce and inspect products.
Q2. How to ensure that every process's quality?
A2:Every process will be checked by our quality inspection department which insures every product's quality. we will personally go to tIn the production of products,he factory to check the quality of products.
Q3.How long is your delivery time?
A3:Our delivery time is generally 30 to 45 days. Or according to the quantity.
Q4. What is your payment method?
A4:30% value of T/T in advance and other 70% balance on B/L copy.
Q5.Can you provide a sample?
A5:Sure, Our sample is provided free of charge, but not including courier fees


Hot Tags: sae1020 astm cold drawn bright round bar ss400 a36 s45c sae1045 42crmo, China sae1020 astm cold drawn bright round bar ss400 a36 s45c sae1045 42crmo suppliers, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar
You Might Also Like
Send Inquiry