30ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars
video

30ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars

36NiCrMo16, 35NCD16, 30NCD16 are permanent chromium-nickel-molybdenum alloy construction steels for the most heavy-duty machine parts, construction and equipment, and for aviation and aerospace industries. These materials (and their substitutes) are characterized by significantly higher nickel content than 36HNM, 34HNM, 38HNM, and thus better tensile strength and yield point. In addition, they exhibit very good hardenability, impact resistance, load, deformation, wear and tensions resistances.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 30ncd16 diameter 8mm 10mm hot rolled steel bars in China. If you're going to wholesale high quality 30ncd16 diameter 8mm 10mm hot rolled steel bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

30ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars

Description

Steel Grade: Alloy Steel 30NCD16 Alloy Or Not: Is Alloy
Technique: Hot Rolled,Forged,Cold Drawn Application: Structural Steel Bar,Die Steel Bar,Tool Steel Bar
Type: Alloy Steel Bar,Carbon Steel Bar,Mold Steel,high Speed Tool Steel Standard: ASTM
Special Use: Mold Steel Shape: Round
Length: 1--12m Surface: Black Or Bright
Surface Treatment: Black/Peeling/Polishing/Machined Diameter: 6-350mm
Heat Treatment: Normalized +Annealed +Quenched + Tempered
High Light:

30ncd16 hot rolled steel bars

,

8mm hot rolled steel bars

,

steel round hot rolled 10mm

Steel 36NiCrMo16, 1.6773, 35NCD16, 30NCD16, 30NiCrMo16, 1.6747 - specification and applications

36NiCrMo16, 35NCD16, 30NCD16 are permanent chromium-nickel-molybdenum alloy construction steels for the most heavy-duty machine parts, construction and equipment, and for aviation and aerospace industries.

These materials (and their substitutes) are characterized by significantly higher nickel content than 36HNM, 34HNM, 38HNM, and thus better tensile strength and yield point. In addition, they exhibit very good hardenability, impact resistance, load, deformation, wear and tensions resistances.

30NiCrMo16 / 1.6747 as the norm itself indicates, has less carbon content. 35NiCrMo16 / 1.2766 grade is classified as a tool steel and is used for the production of special knives or molds for the production of plastics.


Mechanical properties of 36NiCrMo16 steel:

Mechanical properties for individual dimensions
Dimensions: di (mm) 16 - 40mm 40 - 100mm 100 - 160mm 160 - 250mm
Thickness of semi-finished flat product: t (mm) 8 - 20mm 20 - 60mm 60 - 100mm 100 - 160mm
Tensile strength: Rm (MPa) 1250 - 1450 MPa 1100 - 1300 MPa 1000 - 1200 MPa 1000 - 1100 MPa
Yield point: Re (MPa) ≥ 1050 MPa ≥ 900 MPa ≥ 800 MPa ≥ 800 MPa
Notch toughness: KV (J) ≥ 30 J ≥ 35 J ≥ 45 J ≥ 45 J
Elongation: A (%) ≥ 9% ≥ 10% ≥ 11% ≥ 11%
Contraction: Z (%) ≥ 40% ≥ 45% ≥ 50% ≥ 50%

 


36NiCrMo16 steel heat treatment:

Heat treatment of the 36NiCrMo16 grade according to EN 10083-1
Normalizing annealing 850 - 880℃
Softening annealing 650 - 700℃
Hardening 865 - 885℃ w oleju, w wodzie lub oleju
Tempering 550 - 650℃
Hardness in softened state < 269 HB
Density ρ ~7,82 kg/dm3

 


In the 36NiCrMo16, 35NCD16, 30NCD16, 30NiCrMo16 grades we supply:

Round, square, hexagonal hot-rolled bars 36NiCrMo16

Forgings 36NiCrMo16

Drawn and peeled bars 36NiCrMo16

Forged square and round bars 36NiCrMo16

Forged flat bars 36NiCrMo16

30ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars 030ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars 130ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars 230ncd16 Diameter 8mm 10mm Hot Rolled Steel Bars 3