PH 13-8 Mo 1.4534 Stainless Steel Square Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ph 13-8 mo 1.4534 stainless steel square bar in China. If you're going to wholesale high quality ph 13-8 mo 1.4534 stainless steel square bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
PH13-8 Mo Stainless Steel (UNS S13800) square bar is a martensitic precipitation-hardening stainless steel that has excellent strength, high hardness, superior toughness, and good corrosion resistance. Good transverse toughness properties are achieved by tight chemical composition control, low carbon content, and vacuum melting. The alloy is produced by vacuum induction melting (VIM) followed by electro-slag remelting (ESR). As a result of this melt practice, excellent macro- and microcleanliness is achieved, and tight compositional control is implemented.

13-8 MO Stainless Steel Square Bar Chemical Composition
|
C |
Mn |
Si |
Cr |
Ni |
Mo |
Ti |
Al |
– |
|
|
Min |
– |
– |
– |
12.25 |
7.50 |
2.0 |
– |
0.90 |
% |
|
Max |
0.05 |
0.10 |
0.10 |
13.25 |
8.50 |
2.50 |
– |
1.35 |
% |
13-8 MO SS Square Bar Physical Properties
| DENSITY (G/CM 3) |
8.0 |
| DENSITY (LB/IN 3) |
0.289 |
| MELTING POINT (°C) |
1400 – 1455 |
| MELTING POINT (°F) |
2550 – 2650 |
PH13-8Mo is martensitic in structure in the solution annealed condition and is further strengthened by a relatively low temperature heat treatment, which precipitates a strengthening phase in the alloy. Compared to 17-4PH, PH13-8Mo requires only a simple heat treatment, a one step process conducted at a temperature in the range 950°F (510°C) to 1150°F (620°C) depending on the combination of strength and toughness desired.
Further, the alloy has good resistance to stress related corrosion cracking as well, which is why in the alloy functions well in hydrocarbon based industries like the petrochemical industry. In comparison to other high alloyed grades that exhibit resistance to corrosion, the AMS 5629 13-8 MO Hex Bar is manufactured keeping in accordance with the limited acceptability of certain elements. In this case, the limited inclusion of both sulfur and phosphorus in the chemical composition of the UNS S13800 Flat bar, is what manifests a relatively intricate manufacturing process.
Customer Visit
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.
Hot Tags: ph 13-8 mo 1.4534 stainless steel square bar, China ph 13-8 mo 1.4534 stainless steel square bar suppliers, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar
You Might Also Like
Send Inquiry