Hot Rolled With Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM
video

Hot Rolled With Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM

Test: Ultrasonic test according to SEP 1921-84 G3 C/c Certificate of Quality issued in English, in addition the normal terms, production process, the mechanical property (yield strength, tensile strength, elongation and hardness), forged ratio, UT test result, Grain size, heat treatment methods and the sample of is shown on the Certificate of Quality Marking: Grade, heat NO. length will be stamped one each bar with required color Payment: 30% advance by TT; Balance pay before the shipment against shipping documents or irrevocable LC at sight Application: Statically and dynamically stressed components for vehicles, engines and machines. For parts of larger cross-sections, crankshafts, gears.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hot rolled with heat treatment carbon steel round bar c45 sae1045 forged shaft bar 380mm in China. If you're going to wholesale high quality hot rolled with heat treatment carbon steel round bar c45 sae1045 forged shaft bar 380mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hot Rolled With Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MMDescription
Model Number: 45# Material: Carbon Steel Round Bar
Length: 1-6M,9M Technique: Quality
Shaped: Round Application: Construct,shipbuilding,industry
High Light:

forged steel round bar

,

bright steel round bar

 
Hot Rolled With Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM



Round bar steel diameter 20-500mm,material 20#,45#,55#,40CrUP,40CrUC,40Mn2,20CrMnTi,42CrMo
Rolling tube blank diameter 50-130mm.material 20#,45#,10#,35#,37Mn5,Q345,20Mn2/30Mn2,45Mn2,
27SiMn
Casting round tube blank diameter160-230mm,material 20#,45#,25Mn,Q345B,20Mn2/30Mn2,45Mn2,27SiMn,33Mn2V/36Mn2V,
Bearing steel diameter18-60mm,material GCr15,Flat spring steel material 60Si2Mn,55CrMnA,50CrVA

photoes
Hot Rolled With  Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM 0Hot Rolled With  Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM 1

Grade

Dia(mm)

C

Si

Mn

P

S

Ni

Cu

Cr

20


18-600

0.17-0.23

0.17-0.37

0.35-0.65

≤0.035

≤0.035

≤0.30

≤0.25

≤0.25

45

20-600

0.42-0.50

0.17-0.37

0.35-0.65

≤0.035

≤0.035

≤0.30

≤0.25

≤0.25

 

 

Material:

forged square steel bar

Diameter:

100mm-1000mm

Length:

2000mm-12000mm Straightness: 3mm/M max;
square bar.100-1000mm, blocks sizes up to 800*1000mm

Process:

EAF + LF + VD + Forged + Heat Treatment (optional)

Delivery condition:

Hot forged +Rough machined (black surface after Q/T)+ Turned (optional)

Delivery Time:

30-45 days

MOQ:

20 tons

Heat treatment:

Normalized / Annealed / Quenched / tempered

Forged ratio:

no less than 3:1

Technical Data:

According to the customer's requirement of Chemical Composition, Physical Properties and Mechanical Testing

Test:

Ultrasonic test according to SEP 1921-84 G3 C/c

Certificate of Quality

issued in English, in addition the normal terms, production process, the mechanical property (yield strength, tensile strength, elongation and hardness), forged ratio, UT test result, Grain size, heat treatment methods and the sample of is shown on the Certificate of Quality

Marking:

Grade, heat NO. length will be stamped one each bar with required color

Payment:

30% advance by TT; Balance pay before the shipment against shipping documents or irrevocable LC at sight

Application:

Statically and dynamically stressed components for vehicles, engines and machines. For parts of larger cross-sections, crankshafts, gears.



Hot Rolled With  Heat Treatment Carbon Steel Round Bar C45 SAE1045 Forged Shaft Bar 380MM 2

Hot Tags: hot rolled with heat treatment carbon steel round bar c45 sae1045 forged shaft bar 380mm, China hot rolled with heat treatment carbon steel round bar c45 sae1045 forged shaft bar 380mm suppliers, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar