Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of en 10084: 2008 steel round bar din 16mncr5 sh (1.7131) 34 mm bg hot rolled case hardening steel in China. If you're going to wholesale high quality en 10084: 2008 steel round bar din 16mncr5 sh (1.7131) 34 mm bg hot rolled case hardening steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
EN 10084: 2008 Steel Round Bar DIN 16MnCr5 SH (1.7131) 34 mm BG Hot Rolled Case Hardening Steel
Description
| OD: | 6-500mm | Surface: | Black And Bright |
|---|---|---|---|
| Length: | 3-12m | Condition: | Heat Treatment |
| Type: | Hot Rolled | Steel Grade: | Alloy Steel |
| Alloy Or Not: | Is Alloy | Technique: | Hot Rolled,Forged,Cold Drawn |
| Shape: | Round | Surface Treatment: | Black/Peeling/Polishing/Machined |
| Diameter: | 12mm-650mm | Delivery Condition: | Within15 Days After Received The Deposit |
| Dimensions: | 10mm~800mm |
16MnCr5 Steel Round Bar Hot Rolled Alloy Bar EN10084 DIN 1.7131 Special Alloy Rod
| Grade : | 16MnCr5 | ||||
| Number: | 1.7131 | ||||
| Classification: | Alloy special steel | ||||
| Standard: |
|
||||
| Equivalent grades: | Go here |
Chemical composition % of steel 16MnCr5 (1.7131): EN 10084-2008
| Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. Steels with improved machinability as a result of the addition of lead or higher sulfur contents, depending on the manufacturing process up to around 0.1 % S, may be supplied on request. In this case, the upper limit of the manganese content may be increased by 0.15 % |
| C | Si | Mn | P | S | Cr |
| 0.14 - 0.19 | max 0.4 | 1 - 1.3 | max 0.025 | max 0.035 | 0.8 - 1.1 |
Mechanical properties of steel 16MnCr5 (1.7131)
| Nominal thickness (mm): | to 16 |
| Rm - Tensile strength (MPa) hardening and tempering at 200 | 1000 |
| Rm - Tensile strength (MPa) (+A) | 550 |
| Rp0.2 0.2% proof strength (MPa) (+A) | 420 |
| A - Min. elongation Lo = 80 mm (%) (+A) | 21 |
| Z - Reduction in cross section on fracture (%) | 62-64 |
| Brinell hardness (HBW): (+A) | 207 |
| Brinell hardness (HBW): (+TH) | 156 - 207 |
| Brinell hardness (HBW): (+FP) | 140 - 187 |
| Brinell hardness (HBW): (+N) | 138 - 187 |
| Rockwell B hardness ( HRB or RB): (+A) | 84 |
| Vickers hardness ( HV): (+A) | 170 |
Properties of steel 16MnCr5 (1.7131)
| Weldability: It is a MnCr alloy steel, easily hot machinable and weldable Hardenability: It has a low hardenability and therefore it can show good core features till thicknesses of about 20 mm. |
Equivalent grades of steel 16MnCr5 (1.7131)
Warning! Only for reference
| EU EN |
USA - |
Germany DIN,WNr |
France AFNOR |
England BS |
Italy UNI |
Spain UNE |
China GB |
Sweden SS |
Poland PN |
Czechia CSN |
Kazakhstan GOST |
Inter ISO |
|||||||||||||||
| 16MnCr5 |
|
|
|
|
|
|
|
|
|
|
|
|
NEW opportunities for buyers!
Post free buying requirement of steel 16MnCr5 (1.7131)
Mechanical properties
| ReH | Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale |
| Rm | Tensile strength / Zugfestigkeit / Resistance a la traction |
| A | Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal |
| J | Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc |
Heat treatment conditions
|
|
|
Alloy special steel |





Hot Tags: en 10084: 2008 steel round bar din 16mncr5 sh (1.7131) 34 mm bg hot rolled case hardening steel, China en 10084: 2008 steel round bar din 16mncr5 sh (1.7131) 34 mm bg hot rolled case hardening steel suppliers, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar