SUS 416 Metal Rod UNS S41600 Free Cutting Steel Stainless Steel Round Bar OD 50MM
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus 416 metal rod uns s41600 free cutting steel stainless steel round bar od 50mm in China. If you're going to wholesale high quality sus 416 metal rod uns s41600 free cutting steel stainless steel round bar od 50mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
SUS 416 Metal Rod UNS S41600 Free Cutting Steel Stainless Steel Round Bar OD 50MM
Description
| Certification: | ISO,BV,SGS | Type: | Round |
|---|---|---|---|
| Application: | Construction | Standard: | DIN,ASTM,AISI,JIS,EN |
| Grade: | 400 Series 416 | Shape: | Round |
| Special Use: | Valve Steels,Free Cutting Steel | Dimensions: | 5.5mm-500mm |
| Surface: | Bright,Polished,black | Technique: | Cold Rolled Hot Rolled |
| Packing: | Standard Seaworthy Package | Price Term: | CIF CFR FOB Ex-Work |
| High Light: |
SUS 416 Metal Rod,OD 50MM Stainless Steel Bar,SGS Stainless Steel Bar Rod |
||
SUS 416 Metal Rod UNS S41600 Free Cutting Steel Stainless Steel Round Bar OD 50MM
Alloy 416 is a martensitic, free-machining, chromium steel alloy that is generally considered to be the first free-machining stainless steel. It has the highest machinability of any stainless steel at about 85% of that of a free-machining carbon steel. Martensitic stainless steels were designed to be hardenable by heat treatment and also corrosion resistant. Although Alloy 416 and other martensitic stainless steels are not as resistant as austenitic or ferritic stainless, it still demonstrates good corrosion and oxidation resistance plus high strength in the hardened and tempered condition. Alloy 416HT is easily machined, is always magnetic, and has low frictional properties that reduce galling and seizing.
Specifications: UNS S41600
APPLICATIONS:
Alloy 416 is generally used for parts that are extensively machined and require the corrosion resistance of a 13% chromium stainless steel. Applications that generally use Alloy 416 include:
Electrical motors
Nuts and bolts
Pumps
Valves
Automatic screw machine parts
Washing machine components
Studs
Gears
STANDARDS:
ASTM/ASME: UNS S41600
EURONORM: FeMi35Cr20Cu4Mo2
DIN: 2.4660
CORROSION RESISTANCE:
Demonstrates corrosion resistance to natural food acids, waste products, basic and neutral salts, natural waters, and most atmospheric conditions
Less resistant that the austenitic grades of stainless steel and also the 17% chromium ferritic alloys
High sulfur, free-machining grades like Alloy 416 are unsuitable for marine or other chloride exposure
Maximum corrosion resistance is achieved in the hardened condition, with a smooth surface finish
HEAT RESISTANCE
Fair resistance to scaling in intermittent service up to 1400oF (760oC) and up to 1247oF (675oC) in continuous service
Not recommended for use in temperatures above the relevant tempering temperature if maintenance of mechanical properties is important
PROCESSING
WELDING CHARACTERISTICS
Poor weldability
If welding is necessary use Alloy 410 low hydrogen electrodes
Pre-heat to 392 to 572°F (200-300°C)
Follow immediately with annealing or re-hardening, or a stress relief at 1202 to 1247°F (650 to 675°C)
MACHINABILITY
Has outstanding machinability
Best machinability is in the sub-critical annealed condition
PROPERTIES
Chemical Properties:
| C | Mn | Si | P | S | Cr | |
|---|---|---|---|---|---|---|
| 416 | 0.15 max |
1.25 max |
1.00 max |
0.06 max |
0.15 max |
min: 12.0 max: 14.0 |
Mechanical Properties:
| Tempering Temperature (°C) | Tensile Strength (MPa) | Yield Strength 0.2% Proof (MPa) |
Elongation (% in 50mm) |
Hardness Brinell (HB) |
Impact Charpy V (J) |
|---|---|---|---|---|---|
| Annealed * | 517 | 276 | 30 | 262 | – |
| Condition T ** | 758 | 586 | 18 | 248-302 | – |
| 204 | 1340 | 1050 | 11 | 388 | 20 |
| 316 | 1350 | 1060 | 12 | 388 | 22 |
| 427 | 1405 | 1110 | 11 | 401 | # |
| 538 | 1000 | 795 | 13 | 321 | # |
| 593 | 840 | 705 | 19 | 248 | 27 |
| 650 | 750 | 575 | 20 | 223 | 38 |
| * Annealed properties are typical for Condition A of ASTM A582. | |||||
| ** Hardened and tempered Condition T of ASTM A582 – Brinell Hardness is specified range, other properties are typical only. | |||||



Hot Tags: sus 416 metal rod uns s41600 free cutting steel stainless steel round bar od 50mm, China sus 416 metal rod uns s41600 free cutting steel stainless steel round bar od 50mm suppliers, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar