Custom 450 SS Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of custom 450 ss round bar in China. If you're going to wholesale high quality custom 450 ss round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Custom 450 (UNS S45000) is a martensitic age-hardening stainless steel that belongs to the family of precipitation-hardening (PH) alloys. This alloy is known for its exceptional combination of corrosion resistance and high strength, making it suitable for a variety of demanding applications.

Composition and Properties of Custom 450 stainless steel bar:
1. Composition: Custom 450 Round Bar is primarily composed of iron, chromium, nickel, and other elements such as molybdenum, columbium, and copper. The controlled addition of these elements provides the alloy with its unique set of mechanical and corrosion-resistant properties.
2. Mechanical Properties: Custom 450 exhibits excellent mechanical properties, including high tensile strength and hardness. It can be heat-treated to achieve a wide range of strength levels, making it adaptable to different engineering requirements.
3. Corrosion Resistance: One of the standout features of Custom 450 is its resistance to corrosion in various environments. The alloy demonstrates good resistance to both general corrosion and stress corrosion cracking. This makes it particularly suitable for applications in harsh chemical and marine environments.
Custom 450 SS Bars Specification
Dimension : EN, DIN, JIS, ASTM, BS, ASME, AISI
Grade : Custom 450 (UNS No. S45000) Round Bars
Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
Form : Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.
Surface : Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline
Application : Chemical process, Food processing, Petrochemical, Pollution control, Pulp and Paper, Refining
Condition : Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished.
Custom 450 Stainless Round Bar Chemical Composition
| Grade | C | Mn | Si | Ni | Cr | Ti | Mo | Al | Cu |
| Custom 450 | 0.05 max | 1 max | 1 max | 7.5 - 9.5 | 11.0 - 12.5 | .90 - 1.40 | .50 | .75 - 1.50 | 1.5 - 2.5 |
CUSTOMER VISIT
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.
Hot Tags: custom 450 ss round bar, China custom 450 ss round bar suppliers, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes
You Might Also Like
Send Inquiry