ASTM A182 F55 Super Duplex Steel Round Bars
video

ASTM A182 F55 Super Duplex Steel Round Bars

Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) stainless bar has excellent resistance Pitting and Crevice Corrosion in seawater at elevated temperatures, supplied with a PREN 40<( Pitting Resistance Eqv) . Excellent resistance to SCC ( Stress Corrosion Cracking) in Sour and Chloride environments .
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a182 f55 super duplex steel round bars in China. If you're going to wholesale high quality astm a182 f55 super duplex steel round bars made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

The ASTM A182 F55 Super Duplex Stainless Bars is combining very good mechanical strength and good ductility with very good corrosion resistance at ranges of the atmosphere. This grade is provided in annealed condition giving the yielding strength in the excess of 550MPA. This material can't be hardened through the heat treatment but the stronger surface strength can be obtained through the process of cold working. This grade is supplied with the PREn of more than 40 that are guaranteeing greater resistant to the pitting corrosion. Additionally, high resistance to crevice corrosion and stress corrosion is coupled with the high rise strength that provides the alloy greater pros over the other alloys.

Super Duplex ASTM A182 F55 stainless bars are a type of stainless steel that is composed of chromium, nickel, molybdenum, nitrogen, iron and manganese. This particular combination makes the round bar exceptionally resistant to corrosion from high temperatures or pressure as well as from acidic environments. It also offers superior tensile strength as compared to other grades of stainless steel. Super Duplex F55 SS Bars are a common type of steel used in construction and engineering projects. They are highly durable, strong, and can withstand extreme temperatures and pressures. This type of steel is often used in applications where strength and corrosion resistance are required.

super stainless barss rod

 

 

Chemical Composition of ASTM A182 F55 Bars
Grade C Mn Si P S Cr Mo Ni N Fe
F55 0.03 max 2.0 Max 1 Max 0.03 Max 0.02 Max 21 - 23 2.5 - 3.5 4.5 - 6.5 0.80 - 0.20 -

 

ASTM A182 SS F55 Bars Mechanical Properties

0.2% Proof Stress (N/mm2 ) [ksi] minimum 550 550 [79.8]
Ultimate Tensile Strength (N/mm2) [ksi] minimum 750 [108.8]]
Elongation (%) minimum 25
Hardness (HBN) 270max
Reduction of Cross Section Area (%) minimum 45
Charpy V-notch Impact at ambient Temp (J) [ft.lb] 80min [59min]
Charpy V-notch Impact at -46°C (J) [ft.lb] 45av, 35min [33av, 25.8min]

 

Super Duplex Steel F55 Stainless Bars Application Industries:
  • Petrochemical Industry
  • Chemical Industry
  • Oil and Gas Industry
  • Pulp & Paper Indusry
  • Power Plant Industry
  • Food Processing Industry
  • Pharmaceuticals Industry
  • Energy Industry
  • Aerospace Industry

 

Customer Visit

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

gnee steelgnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: astm a182 f55 super duplex steel round bars, China astm a182 f55 super duplex steel round bars suppliers, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry