A286 Stainless Steel Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of a286 stainless steel bar in China. If you're going to wholesale high quality a286 stainless steel bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
A-286 SS bar can still be cold-worked with satisfactory results. When compared with other nickel or cobalt-based high-temperature alloys A-286 is considerably easier to machine. It can also be solution annealed and age hardened for various applications, and is often treated to provide superior creep strength. GNEE Steel offers a number of value-added surfaces, including age hardening and solution annealing.

A286 Stainless Steel Applications
- Jet engine components
- High-temperature turbine wheels and blades
- High-temperature frames
- High-temperature casings
- Gas turbine, disks, blades & shafts
- Compressors
- Manifold Components
- Tanks, pumps, piping, valves, and heat exchange
- High-temperature afterburner parts
- High-temperature fasteners, springs
- Non-magnetic cryogenic equipment
- Superchargers
Stainless Steel Alloy A286 Bar Chemical Composition
| CHEMICAL COMPOSITION | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Ni 52.5% | Cr 19% | Nb 5.125% | Mo 3.05% | Co <=1% | |||||
| Ti 0.90% | Si <=0.35% | Mn <=0.35% | Cu <= 0.30% | Al 0.50% | |||||
| C <=0.08% | Ta <=0.05% | B <=0.006% | P <= 0.015% | S <=0.015% | |||||
| Fe balance | |||||||||
Alloy A286 Stainless Rod Physical Properties
| PHYSICAL PROPERTIES | ||||||
|---|---|---|---|---|---|---|
| Density | Electrical conductivity (% IACS) | Thermal conductivity (BTU-in/hr-ft²-°F) | Specific heat capacity | Thermal expansion (1/°F) | Melting Point (°F) | |
| 0.286 | 1.9 | 104 | 0.11 | 0.00000917 | 2500 | |
Grade A286 SS Bar Mechanical Properties
| MECHANICAL PROPERTIES | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| PROPERTY | MINIMUM | MAXIMUM | |||||||
| Yield Strength Range (Rp0.2 Offset) (ksi) | 50 | 95 | |||||||
| Tensile Strength Range (Rm) (ksi) | 90 | 171 | |||||||
| Elongation (AL=5 x Ø) | 11.0% | 24.0% | |||||||
| Brinell Hardness (H) | 279 | 327 | |||||||
| Modulus of Elasticity (ksi) (E): 29000 | |||||||||
| Machineability General Index: 28% | |||||||||
Customer Visit
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.
Hot Tags: a286 stainless steel bar, China a286 stainless steel bar suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar
Previous
SS904L Stainless Steel RodYou Might Also Like
Send Inquiry