Alloy Polished 25mmDIN1.4125 Stainless Steel Round Bar UNS S44000 SUS 440C
video

Alloy Polished 25mmDIN1.4125 Stainless Steel Round Bar UNS S44000 SUS 440C

Preheat to 760oC – 820oC, then heat slowly and uniformly to 1050oC – 1150oC, hold until temperature is uniform throughout the 440c steel section and commence forging immediately. Do not overheat 440c stainless steel as this can cause a loss of toughness and ductility. Do not forge below 900oC. Finished forgings of SS 440c should be cooled slowly in a furnace, warm dry lime or ashes to room temperature and annealed immediately. Air cooling after forging may cause cracking of steel 440c.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy polished 25mmdin1.4125 stainless steel round bar uns s44000 sus 440c in China. If you're going to wholesale high quality alloy polished 25mmdin1.4125 stainless steel round bar uns s44000 sus 440c made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy Polished 25mmDIN1.4125 Stainless Steel Round Bar UNS S44000 SUS 440C

Description

Certification: ISO,BV,SGS Surface: Bright / Black 2B NO.1
Thickness: 1-100mm Width: 100-1220mm
Length: Customers' Requirements Standard: DIN,ASTM,AISI,JIS,EN
Grade: 400 Series Technique: Cold Rolled Hot Rolled
Packing: Standard Seaworthy Package Price Term: CIF CFR FOB Ex-Work
High Light:

Alloy Polished Stainless Steel Bar

,

UNS S44000 Stainless Steel Bar

,

25mm 440C Stainless Steel Bar

Raw Material Alloy 440C UNS S44000 DIN1.4125 SUS 440C Black Polished 25mm Stainless Steel Round Bar

 

Stainless steels are high-alloy steels which have high corrosion resistance compared to other steels due to the presence of large amounts of chromium. Based on their crystalline structure, they are divided into three types such as ferritic, austenitic, and martensitic steels. Another group of stainless steels are precipitation-hardened steels. They are a combination of martensitic and austenitic steels.

Grade 440C stainless steel is a high carbon martensitic stainless steel. It has high strength, moderate corrosion resistance, and good hardness and wear resistance. Grade 440C is capable of attaining, after heat treatment, the highest strength, hardness and wear resistance of all the stainless alloys. Its very high carbon content is responsible for these characteristics, which make 440C particularly suited to such applications as ball bearings and valve parts.

APPLICATIONS

Typical applications include:

Rolling element bearings

Valve seats

High quality knife blades

Surgical instruments

Chisels

SPECIFICATIONS

UNS: ASTM/ASTE S44000

DIN: 1.4125

 

Name stainless steel round bar material 440C
OD size 10-250mm Length 6m
surface polished / black standard ASTM A276

AISI 440C is a high-carbon chromium steel designed to provide stainless properties with maximum hardness. It has been used primarily as a bearing steel, and is used in the hardened plus tempered condition. When heat-treated, Type 440C attains the highest hardness of any stainless steel (about Rockwell C 60).

Typical applications are bearing assemblies, including bearing balls and races. In addition, it should be considered for cutlery, needle valves, ball check valves, valve seats, pump parts, ball studs, bushings, and wear-resistant textile component

 

Supply Range for 440C Stainless Steel

 

440C steel round bar: diameter 1mm~400mm

440C stainless plate: 0.1-100 thickness x 500-2000mm width x 1000-6000mm length

Other steel shape, like 440c steel sheet, 440C coil, flat bar and customized sizes are available against request

Standard of 440C Stainless Steel and Equivalent Steel Grades

Country USA BS & DIN Japan
Standard ASTM A276 EN 10088 JIS G4303
Grades S44004/440C X105CrMo17/1.4125 SUS440C

ASTM A276 440C Steel Chemical Composition and Equivalent's

Standard Grade C Mn P S Si Cr Mo
ASTM A276 S44004/440C 0.95-1.20 ≦1.00 ≦0.04 ≦0.03 ≦1.00 16.0-18.0 ≦0.75
EN10088 X105CrMo17/1.4125 0.95-1.20 ≦1.00 ≦0.04 ≦0.03 ≦1.00 16.0-18.0 0.40-0.80
JIS G4303 SUS 440C 0.95-1.20 ≦1.00 ≦0.04 ≦0.03 ≦1.00 16.0-18.0 ≦0.75

ASTM 440C Stainless Steel Mechanical Properties

Tempering Temperature (°C) Tensile Strength (MPa) Yield Strength 0.2% Proof (MPa) Elongation (% in 50mm) Hardness Rockwell (HRC) Impact Charpy V (J)
Annealed* 758 448 14 269HB max# –
204 2030 1900 4 59 9
260 1960 1830 4 57 9
316 1860 1740 4 56 9
371 1790 1660 4 56 9

Physical Properties

Grade Density (kg/m3) Elastic Modulus (GPa) Mean Coefficient of Thermal Expansion (mm/m/°C) Thermal Conductivity(W/m.K) Specific Heat Electrical Resistivity (nW.m)
0-100°C 0-200°C 0-600°C at 100°C at 500°C 0-100°C (J/kg.K)
440 C 7650 200 10.1 10.3 11.7 24.2 – 460 600

Forging of 440C Stainless Steel

Preheat to 760oC – 820oC, then heat slowly and uniformly to 1050oC – 1150oC, hold until temperature is uniform throughout the 440c steel section and commence forging immediately. Do not overheat 440c stainless steel as this can cause a loss of toughness and ductility. Do not forge below 900oC. Finished forgings of SS 440c should be cooled slowly in a furnace, warm dry lime or ashes to room temperature and annealed immediately. Air cooling after forging may cause cracking of steel 440c.

Machinability of 440C Steel

ASTM Grade 440C stainless steel can be machined well, with all operations such as turning and drilling etc., in the annealed condition. Because of 440C SS high carbon content it machines somewhat like high-speed steel. Because chips are tough and stringy, chip curlers and breakers are important.

As heat treated, the 440 steel series are difficult to machine because of their high hardness. For parts that require extensive machining, the free-machining versions, Type 440F or Type 440F Se, offer improved machining properties.

 

Alloy Polished 25mmDIN1.4125 Stainless Steel Round Bar UNS S44000  SUS 440C 0Alloy Polished 25mmDIN1.4125 Stainless Steel Round Bar UNS S44000  SUS 440C 1

Hot Tags: alloy polished 25mmdin1.4125 stainless steel round bar uns s44000 sus 440c, China alloy polished 25mmdin1.4125 stainless steel round bar uns s44000 sus 440c suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry