SUS439 Stainless Steel Plate S43940 DIN1.4510 Size 5x20Ft 5mm Surface
video

SUS439 Stainless Steel Plate S43940 DIN1.4510 Size 5x20Ft 5mm Surface

Type 439 is an 18% chromium, titanium stabilized ferritic stainless steel with corrosion resistance similar to that of 304/304L stainless steel. This grade may be used in the annealed, cold formed or as-welded condition in applications where other stainless steels such as Type 304/304L and Type 430 are used. Type 439 has good weldability due to titanium stabilization and has excellent resistance to stress corrosion cracking. Type 439 outperforms Type 409 in both oxidation and corrosion resistance and typical applications include tubular manifolds and exhaust system components.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus439 stainless steel plate s43940 din1.4510 size 5x20ft 5mm surface in China. If you're going to wholesale high quality sus439 stainless steel plate s43940 din1.4510 size 5x20ft 5mm surface made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SUS439 Stainless Steel Plate S43940 DIN1.4510 Size 5x20Ft 5mm Surface

Description

Material: Metal Plate Metal Type: Stainless Steel
Usage Condition: FLOOR,Desktop,Hanging Size: Customized Size 1219*2438mm 1500*6000mm
Thickness: 1-100mm Shape: Flat Plate
High Light:

SUS439 Stainless Steel Plate

,

DIN1.4510 Stainless Steel Plate

,

ferritic Stainless Steel Metal Plate

Stainless Steel Plate SUS439 DIN1.4510 Size 5x20Ft 5mm(Thick) Surface No.1

Type 439 (UNS S43035)

Description
Type 439 is an 18% chromium, titanium stabilized ferritic stainless steel with corrosion resistance similar to that of 304/304L stainless steel. This grade may be used in the annealed, cold formed or as-welded condition in applications where other stainless steels such as Type 304/304L and Type 430 are used. Type 439 has good weldability due to titanium stabilization and has excellent resistance to stress corrosion cracking. Type 439 outperforms Type 409 in both oxidation and corrosion resistance and typical applications include tubular manifolds and exhaust system components.

 

Chemical Composition
Chemical Composition (wt%) limits as specified in ASTM A240 and ASME SA240*

 

Element 439
Carbon 0.030
Chromium 17.0-19.0
Nickel 0.50
Manganese 1.00
Silicon 1.00
Nitrogen 0.030
Phosphorus 0.040
Sulfur 0.030
Aluminum 0.15

 

Titanium

0.20 +4(C+N) min
1.10 max

 

 

Mechanical Properties

Mechanical property requirements for annealed product as specified in ASTM A240 and ASME SA240

Property 439
Yield Strength, min. (ksi) 30
Tensile Strength, min. (ksi) 60
Elongation, min. (%) 22
Hardness, max. (Rb) 89

 

Physical Properties
Physical properties for Type 439 stainless steel

Property 439
Density, lb/in3 0.278
Modulus of Elasticity, psi 29.0 x 106
Coefficient of Thermal Expansion, 68-212˚F, /˚F 5.6 x 10-6
Thermal Conductivity, Btu/ft hr ˚F 14.0
Specific Heat, Btu/lb ˚F 0.11
Electrical Resistivity, Microohm-in 24.8

 

RFQ

 

Q1: Can I get some samples?
A: Yes, we can supply free sample, but the shipping cost should be paid by our customers.
Q2: How to make payments?
A: 30% T/T in advance , the balance before shippment.
Q3: How to confirm the Product Quality before placing orders?
A:You can get free samples for some products,you only need to pay the shipping cost or arrange a courier to us and take the samples. The third-party will be accepted.
Q4:What's your MOQ?
A:Our MOQ is 1.5 ton.
Q5: How about delivery lead time?
A:Delivery lead time: About 7-15 days after payment confirmed.
Q6:Is there a discount?
A:Different quantity has different discount.
 

 

 

SUS439 Stainless Steel Plate S43940 DIN1.4510 Size 5x20Ft 5mm Surface 0SUS439 Stainless Steel Plate S43940 DIN1.4510 Size 5x20Ft 5mm Surface 1

Hot Tags: sus439 stainless steel plate s43940 din1.4510 size 5x20ft 5mm surface, China sus439 stainless steel plate s43940 din1.4510 size 5x20ft 5mm surface suppliers, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, SS431 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry