UNS S31653 Stainless Steel Flat Plate 1.4429 SA 240 Gr.316LN
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns s31653 stainless steel flat plate 1.4429 sa 240 gr.316ln in China. If you're going to wholesale high quality uns s31653 stainless steel flat plate 1.4429 sa 240 gr.316ln made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
UNS S31653 Stainless Steel Flat Plate 1.4429 SA 240 Gr.316LN
Description
| Material: | Stainless Steel | Finishing: | NO.1 2B |
|---|---|---|---|
| Size: | 1000-2000mm Customized Size | Shape: | Flat Plate |
| Feature: | Corrosion Resistance | Thickness: | 1.5-30 Mm Or Customized |
| High Light: |
UNS S31653 Stainless Steel Plate,1.4429 Stainless Steel Plate,Stainless Steel Flat Plate 30mm |
||
Introduction
Stainless steel grade 316LN is an austenitic type of steel that is a low carbon, nitrogen-enhanced version of grade 316 steel. The nitrogen content in this steel provides solid solution hardening, and raises its minimum specified yield strength. It also possesses good resistance to general corrosion and pitting/crevice corrosion.
The following datasheet provides an overview of stainless steel grade 316LN.
SA240 316LN, SA240 TP 316LN, SS 316LN Plate, TP316LN
Mittel is the large manufacturer to supply SA240 316LN,SA240 TP 316LN,
SS 316LN Stainless plate,TP316LN as per ASTM, ASME, JIS , EN, UNS Specs. We have about
3000tons each thickness and size stainless plates and large warehouse. If you have any
requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: SA240 316LN, SA240 TP 316LN, SS 316LN Stainless plate,SS316LN, ASME SA240 316LN,TP316LN
| Product Name | 316LN Stainless Steel Plate |
| Thickness | 0.1-200mm |
| Length | 3000mm,5800mm,6000mm,9000mm,12000mm,etc. |
| Diameter | 3-1220mm |
| Standard | ASTM,JIS, AISI, GB, DIN, EN |
| Surface | BA,2B,NO.1,NO.4,4K,HL,8K |
| Certification | ISO, SGS |
| Technique | Cold Rolled Hot Rolled |
| Edge | Mill Edge Slit Edge |
| Quality | SGS Inspection |
| Grade (ASTM UNS) | 201,304,304L,321,316,316L,317L,347H,309S,310S,904L, S32205,2507,254SMOS,32760,253MA,N08926,etc |
| Payment Terms | T/T L/C and Western Union etc |
| 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) 24-26CBM | |
| 40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High) 54CBM | |
|
40ft HC:12032mm(Length)x2352mm(Width)x2698mm(High) 68CBM |
|
What forms of SA240 316LN Stainless Steel are available at MittelSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
SA240 316LN Chemical Composition, max %
| C | Mn | P | S | Si | Cr |
| 0.03 | 2.00 | 0.045 | 0.030 | 0.75 | 16.0-18.0 |
| Ni | Mo | N | Cu | Others | |
| 10.0-14.0 | 2.00-3.00 | 0.10-0.16 | |||
SA240 316LN Mechanical Properties
| Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB | |
| SA240 TP 316LN | 515 | 205 | 40 | 95 |
Mittel is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.



Hot Tags: uns s31653 stainless steel flat plate 1.4429 sa 240 gr.316ln, China uns s31653 stainless steel flat plate 1.4429 sa 240 gr.316ln suppliers, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate
You Might Also Like
Send Inquiry