SS 321 Stainless Steel Sheet And Plate
video

SS 321 Stainless Steel Sheet And Plate

Type 321 Stainless Steel is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition of at least five times the carbon content. This titanium addition reduces or prevents carbide precipitation during welding and in 800 – 1500°F service. It also improves the elevated temperature properties of the alloy.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 321 stainless steel sheet and plate in China. If you're going to wholesale high quality ss 321 stainless steel sheet and plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Type 321 Stainless Steel is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition of at least five times the carbon content. This titanium addition reduces or prevents carbide precipitation during welding and in 800 – 1500°F service. It also improves the elevated temperature properties of the alloy. Type 321 provides excellent resistance to oxidation and corrosion and possesses good creep strength. It is used primarily in applications involving continuous and intermittent service temperatures within the carbide precipitation range of 800 – 1500°F.

4 359 -

Element Type 321
Carbon 0.08 max.
Manganese 2.00 max.
Sulfur 0.030 max.
Phosphorus 0.045 max.
Silicon 0.75 max.
Chromium 17.00 – 19.00
Nickel 9.00 – 12.00
Titanium 5x(C+N) min. – 0.70 max.
Nitrogen 0.10 max.

Hot Tags: ss 321 stainless steel sheet and plate, China ss 321 stainless steel sheet and plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS409 Stainless Steel Welded Pipe