310 And 310S Stainless Steel
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 310 and 310s stainless steel in China. If you're going to wholesale high quality 310 and 310s stainless steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Types 310 Stainless Steel and 310S are typically used for elevated temperature applications. Their high nickel and chromium contents impart excellent elevated temperature strength and resistance to oxidation compared to Type 304 SS. Type 310S Stainless Steel is identical to Type 310 except for a lower carbon content that minimizes carbide precipitation and improves weldability. They are essentially nonmagnetic as annealed and become lightly magnetic when cold worked.

| Element | Type 310 | Type 310S |
|---|---|---|
| Carbon | 0.25 max. | 0.08 max. |
| Manganese | 2.00 max. | 2.00 max. |
| Sulfur | 0.030 max. | 0.030 max. |
| Phosphorus | 0.045 max. | 0.045 max. |
| Silicon | 1.50 max. | 1.50 max. |
| Chromium | 24.0 – 26.0 | 24.0 – 26.0 |
| Nickel | 19.0 – 22.0 | 19.0 – 22.0 |
SS 310: This grade has a higher carbon content, providing greater strength at elevated temperatures. However, it may be less ductile compared to SS 310S.
SS 310S: This is a low-carbon version of SS 310, offering improved weldability and reduced risk of carbide precipitation during welding. It is preferred for applications requiring both high-temperature resistance and ease of fabrication.
Hot Tags: 310 and 310s stainless steel, China 310 and 310s stainless steel suppliers, Corrugated SS Roof Sheet, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate